Homopolymer and FDA compliant. Features: Exceptional draw down and processability even to 1/2 mil; excellent strength, good heat sealability, and good optical. FDA Notes: Conforms to FDA regulation 21 CFR 177.1520 (c)2.2 under condition of use B through H described in Table 2 of 21 CFR 176.170 Film properties based on 1.0 guage (25 µm) thickness; blow-up ratio 2:1. Information provided by Huntsman Corporation |