MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

3M Scotch-Weld™ RT3500B Rubber-Toughened Instant Adhesive
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: 3M™ Scotch-Weld™ Rubber Toughened Instant Adhesives are formulated with a unique elastomer that maximizes impact, vibration, peel, and thermal cycling resistance while providing tough flexible bonds. These adhesives are ideally suited for bonding flexible substrates and dissimilar materials.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³
Brookfield Viscosity 1000 - 3000 cP1000 - 3000 cPRVT #3 sp @ 20 rpm
 5000 - 10000 cP5000 - 10000 cPRVT #3 sp @ 2.5 rpm
 
Mechanical PropertiesMetricEnglishComments
Shear Strength 8.96 MPa1300 psicured, grit-blasted steel; ASTM D1002
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 93.0 °C199 °FContinuous
 121 °C250 °FIntermittent
Minimum Service Temperature, Air -54.0 °C-65.2 °FContinuous
 -54.0 °C-65.2 °FIntermittent
 
Processing PropertiesMetricEnglishComments
Cure Time 0.333 - 1.50 min0.00555 - 0.0250 hourTime to Handling Strength
 1440 min24.0 hourFull Cure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM34719 / 169466

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.