MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Zoltek™ PX35 Carbon Fiber Prepreg Tape
Categories: Polymer; Thermoset; Carbon Fiber/Thermoset Composite

Material Notes: ZOLTEK produces uni-directional (UD) prepreg tapes based on ZOLTEK carbon fiber. ZOLTEK prepreg is ideal for large-volume composite applications where high production throughput, excellent composite properties, and low material cost are important. A wide selection of epoxy resin formulations (28 tp 45 % (wt/wt)) meets most processing and composite property requirements for tack, toughness, surface finish, cure time, cure temperature, and delivered composite strength and modulus. Custom formulations are also available. Packaging options include core size, customer specified knitting requirements, and custom labeling. ZOLTEK prepreg production is geared to large volumes and low cost.

APPLICATIONS: Wind energy, automotive, petroleum production, aviation, marine, industrial, other transportation, medical (including X-ray), sports and recreation, etc. Excellent for hand layup or automated fabrication processes.

Mechanical properties reported are typical but vary with resin system, loading, cure cycle, etc.

Information provided by Zoltek Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 1850 MPaDIN EN ISO 527
Tensile Modulus 130 GPaDIN EN ISO 527
Compressive Strength 1320 MPaDIN EN ISO 14126
Compressive Modulus 125 GPaDIN EN ISO 14126
Shear Modulus 4.80 GPa+/-45 in plane; DIN EN ISO 14129
Shear Strength 59.0 MPa+/-45 In Plane; DIN EN ISO 14129
 70.0 MPaInterlaminer; ASTM D2344
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 120 °CDMA
 
Descriptive Properties
Areal Weight150 to 600 g/m2
Roll LengthUp to 1500 m or 1000 lb net prepreg weight.
Roll WidthUp to 127 cm.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay CYCOM® 2040 Epoxy Prepreg Fabric with 6KM46J-2X2T-200
Solvay CYCOM® 5250-4 BMI Prepreg System with IM-7 Carbon Fiber
Solvay CYCOM® 2020 Epoxy + M46J 140 Unidirectional Tape Prepreg, with Post-Cure
Solvay CYCOM® 2020 Epoxy + M46J 140 Unidirectional Tape Prepreg, without Post-Cure
Solvay CYCOM® 2040 Epoxy Prepreg Fabric with 6KT800-2X2T-200

PZOL849 / 232327

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.