MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Sandvik 11RM10 Spring wire
Categories: Metal; Ferrous Metal; Stainless Steel

Material Notes: Sandvik 11RM10 is an austenitic stainless steel alloyed with manganese that is characterized by high wear resistance. The grade is normally delivered in flat rolled, hard condition. Sandvik 11RM10 is primarily used for expander rings in automotive engines.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 760 - 1380 MPa110000 - 200000 psiFlat rolled wire
 1100 - 1300 MPa160000 - 189000 psiTypical values
Tensile Strength, Yield  275 - 1170 MPa
@Strain 0.2 %
39900 - 170000 psi
@Strain 0.2 %
Flat rolled wire
 950 - 1200 MPa
@Strain 0.2 %
138000 - 174000 psi
@Strain 0.2 %
Typical values
Modulus of Elasticity 180 GPa26100 ksi
Poissons Ratio 0.290.29Calculated
Shear Modulus 70.0 GPa10200 ksi
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.90 %0.90 %
Chromium, Cr 16.5 %16.5 %
Manganese, Mn 6.4 %6.4 %
Nickel, Ni 4.0 %4.0 %
Nitrogen, N 0.10 %0.10 %
Phosphorus, P <= 0.030 %<= 0.030 %
Silicon, Si 0.50 %0.50 %
Sulfur, S <= 0.010 %<= 0.010 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for T 300 Series Stainless Steel
302 Stainless Steel, annealed strip
301 Stainless Steel
Sandvik 11R51 Spring Wire
Crucible Steel AISI 6150 Alloy Steel

NSANDV5064 / 199628

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.