MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sandvik Kanthal 140 R 140 Thermostatic bimetal
Categories: Metal; Superalloy; Iron Base

Material Notes: KANTHAL 140 R 140 is a thermostatic bimetal which is recommended for use in the temperature range -20 to +250°C.

Typical applications for KANTHAL 140 R 140 are in circuit breakers, motor protection units, thermostats, shower mixers, etc.

High-expansive component: 74-24-1 Alloy (410 Designation, 81% of thickness)

Low-expansive component: Invar 155 Alloy (450 Designation, 19% of thickness)

Information provided by Sandvik

Composition:

  • High-expansive component: Designation 410; 74% Mn; 24.5% Ni; 1% Cu
  • Low-expansive component: Designation 450; 0.12% Mn; 36.8% Ni; Bal. Fe
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.40 g/cc0.267 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 120120High-expansive component
 130130Low-expansive component
 200200Low-expansive component, Cold-worked 20%
 230230High-expansive component, Cold-worked 20%
Tensile Strength, Ultimate 450 MPa65300 psiLow-expansive component
 540 MPa78300 psiHigh-expansive component
Tensile Strength, Yield 260 MPa37700 psiHigh-expansive component
 290 MPa42100 psiLow-expansive component
Elongation at Break 40 %40 %Low-expansive component
 50 %50 %High-expansive component
Modulus of Elasticity 130 GPa18900 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity  0.000138 ohm-cm
@Temperature 0.000 °C
0.000138 ohm-cm
@Temperature 32.0 °F
Bimetal
 0.000148 ohm-cm
@Temperature 200 °C
0.000148 ohm-cm
@Temperature 392 °F
Bimetal
 0.000152 ohm-cm
@Temperature 300 °C
0.000152 ohm-cm
@Temperature 572 °F
Bimetal
 
Thermal PropertiesMetricEnglishComments
CTE, linear  0.500 µm/m-°C
@Temperature 30.0 - 130 °C
0.278 µin/in-°F
@Temperature 86.0 - 266 °F
 26.9 µm/m-°C
@Temperature 30.0 - 130 °C
14.9 µin/in-°F
@Temperature 86.0 - 266 °F
High-expansive component
Specific Heat Capacity 0.460 J/g-°C
@Temperature 20.0 °C
0.110 BTU/lb-°F
@Temperature 68.0 °F
Thermal Conductivity 4.00 W/m-K
@Temperature 20.0 °C
27.8 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Maximum Service Temperature, Air 330 °C626 °F
Minimum Service Temperature, Air -20.0 °C-4.00 °F
 
Descriptive Properties
Linearity Range, °C-20 to 200
linearity Temperature Range, °C-20 to 250
Specific thermal curvature, /K0.0000261
Specific deflection, /K0.000014

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zirconium Oxide, Zirconia, ZrO2
Overview of materials for Aluminum Alloy
General Plastics LAST-A-FOAM® FR-10118 Polyurethane Foam
Alumina, alpha Al2O3, 99.5%
Alliance BCN-10 Bonded (Composite) Magnetic Material

NSANDV112 / 19006

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.