MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
RTP Company EMI 681  Acrylonitrile Butadiene Styrene (ABS) Shielding - Nickel-Coated Carbon Fiber 10%  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), NCG Fiber Filled

Material Notes: Shielding - Nickel-Coated Carbon Fiber 10%

Comments:

  • EMI/RFI Shielding
  • ESD Protection
  • Nickel-Coated Carbon Fiber

Unless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.

Information provided by RTP Company.


Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.14 g/ccASTM D792
Filler Content 10 %
Water Absorption 0.20 %24 hours at 23°C; ASTM D570
Linear Mold Shrinkage 0.0010 - 0.0020 cm/cm
@Thickness 3.17 mm
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 9000 psiASTM D638
Elongation at Break 1.5 %ASTM D638
Modulus of Elasticity 1100 ksiASTM D638
Flexural Yield Strength 14000 psiASTM D790
Flexural Modulus 800 ksiASTM D790
Izod Impact, Notched 1.40 ft-lb/in
@Thickness 3.17 mm
ASTM D256
Izod Impact, Unnotched 4.00 ft-lb/in
@Thickness 3.17 mm
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity <= 1.00 ohm-cmASTM D257
Surface Resistance <= 1e+05ASTM D257
Static Decay <= 2.0 secFTMS-4046.1
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 28.0 µin/in-°F
@Temperature 20.0 °C
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 230 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 220 °FASTM D648
Flammability, UL94 HB
@Thickness 1.59 mm
Per testing by RTP Company; ASTM D635
 
Processing PropertiesOriginal ValueComments
Processing Temperature 410 - 460 °F
Mold Temperature 150 - 180 °F
Injection Pressure 10000 - 15000 psi
 
Descriptive Properties
ColorNatural/Black

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RTP Company ESD 2587 Polycarbonate/ABS Alloy (PC/ABS); Carbon Fiber - Electrically Conductive - ESD Protection
RTP Company ESD 289 Nylon 6/6 (PA); Carbon Fiber - Electrically Conductive
RTP Company EMI 1063 Polybutylene Terephthalate (PBT); Stainless Steel Fiber - EMI/RFI Shielding - Electrically Conductive
RTP Company EMI 1062 Polybutylene Terephthalate (PBT), Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection
RTP Company EMI 1363 Polyphenylene Sulfide (PPS), Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection

PR5532 / 64917

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.