MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Hexcel® HexPly® M77CS Fast Curing Epoxy Resin Matrix
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: HexPly® M77CS is a fast curing hotmelt, thermosetting epoxy matrix, specifically designed for prepreg applications at which short cure cycles and clear surfaces are required. M77CS is recommended for curing at 120 – 150°C and is suitable for a range of pressures (5 – 35bar). M77CS can be used for manufacture of industrial components with a clear surface.

Information provided by Hexcel Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 - 1.25 g/cc0.0415 - 0.0452 lb/in³
Viscosity  1000 cP
@Temperature 110 °C
1000 cP
@Temperature 230 °F
5°C/min
 1.00e+8 cP
@Temperature 25.0 °C
1.00e+8 cP
@Temperature 77.0 °F
5°C/min
 1.00e+8 cP
@Temperature 135 °C
1.00e+8 cP
@Temperature 275 °F
5°C/min
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 125 - 135 °C257 - 275 °FOptimum cured, following a 15min cure @130°C
 
Processing PropertiesMetricEnglishComments
Cure Time  <= 1.50 min
@Temperature 150 °C
<= 0.0250 hour
@Temperature 302 °F
time to 95% conversion; ISO 11357-5
 <= 3.00 min
@Temperature 140 °C
<= 0.0500 hour
@Temperature 284 °F
time to 95% conversion; ISO 11357-5
 <= 6.00 min
@Temperature 130 °C
<= 0.100 hour
@Temperature 266 °F
time to 95% conversion; ISO 11357-5
 <= 9.00 min
@Temperature 120 °C
<= 0.150 hour
@Temperature 248 °F
time to 95% conversion; ISO 11357-5
Shelf Life  1.50 Month
@Temperature 23.0 °C
1.50 Month
@Temperature 73.4 °F
 6.00 Month
@Temperature 5.00 °C
6.00 Month
@Temperature 41.0 °F
 18.0 Month
@Temperature -18.0 °C
18.0 Month
@Temperature -0.400 °F
 
Descriptive Properties
ColorTranslucent/Off white

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHEXCB9153 / 322309

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.