MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Thermal Ceramics Therm-O-Flake Coating
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Therm-O-Flake Coating and Therm-O-Flake Coating-M are lightweight, “fine grained”, gun-applied insulation. They both have an effective temperature range up to 1800°F (982°C). Highly efficient insulations, these coatings are used extensively to reduce radiation loss and air infiltration as well as conserve heat. Therm-O-Flake Coating or Therm-O-Flake Coating-M may be applied to hot or cold surfaces on primary and secondary regenerator walls of glass tanks, reverberatory furnaces, bulkheads, end walls, side walls and arches. They are both particularly effective when used as a sealant over older firebrick walls, bulkheads and arches.

Features:

  • Effective temperature range up to 1800°F
  • Highly efficient insulation
  • Used to reduce radiation loss and air infiltration
  • Applications:

  • Roof/curved surfaces
  • End and side walls
  • Information provided by Thermal Ceramics

    Data has not been recently verified. Please contact manufacturer for current information.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Thermal PropertiesMetricEnglishComments
    Specific Heat Capacity 0.220 J/g-°C0.0526 BTU/lb-°F
    Thermal Conductivity  0.127 W/m-K
    @Temperature 204 °C
    0.880 BTU-in/hr-ft²-°F
    @Temperature 400 °F
    ASTM C201
     0.157 W/m-K
    @Temperature 427 °C
    1.09 BTU-in/hr-ft²-°F
    @Temperature 800 °F
    ASTM C201
     0.189 W/m-K
    @Temperature 649 °C
    1.31 BTU-in/hr-ft²-°F
    @Temperature 1200 °F
    ASTM C201
     0.225 W/m-K
    @Temperature 871 °C
    1.56 BTU-in/hr-ft²-°F
    @Temperature 1600 °F
    ASTM C201
    Maximum Service Temperature, Air 982 °C1800 °F
     
    Component Elements PropertiesMetricEnglishComments
    Al2O3 19 %19 %
    Alkalis 6.8 %6.8 %
    CaO 2.9 %2.9 %
    Fe2O3 6.2 %6.2 %
    MgO 15 %15 %
    SiO2 50 %50 %
     
    Descriptive Properties
    Cr2O3 contenttraces
    Mn2O3 contenttraces
    TiO2 contenttraces

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    CTHERM253 / 2573

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.