MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Go Yen Chemical GOYENCHEM-PTFE Anti-dripping Agent
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: GOYENCHEM-PTFE, anti-dropping flame retardant, is provided by GO YEN CHEMICAL INDUSTRIAL CO., LTD. (GYC GROUP), that work with GY-FR-OP series. When adding into Thermoplastic plastic, due to heat effect, it will generate GOYENCHEM-PTFE microball, which more than 0.18µm, and form cross-link network in the process of pressing and cutting. When burned, this network will contract, then consequently, trap the melted polymer, insulate oxygen, accelerate the carbonization of polymer, and therefore, makes the polymer flame-retarded. GY-PTFE own high Mw PTFE that can effectively fiberize and easily disperse into small particle to meet the antidrip purpose.

Intro: GOYENCHEM-PTFE, anti-dropping flame retardant, is provided by GO YEN CHEMICAL INDUSTRIAL CO., LTD. (GYC GROUP), that work with GY-FR-OP series. When adding into Thermoplastic plastic, due to heat effect, it will generate GOYENCHEM-PTFE microball, which more than 0.18µm, and form cross-link network in the process of pressing and cutting. When burned, this network will contract, then consequently, trap the melted polymer, insulate oxygen, accelerate the carbonization of polymer, and therefore, makes the polymer flame-retarded. GY-PTFE own high Mw PTFE that can effectively fiberize and easily disperse into small particle to meet the antidrip purpose.

Advantages:

  • good anti dropping effect
  • GOYENCHEM-PTFE with high purity and 100% activity
  • great thermal stability
  • good dispersion
  • low dosage
  • high competity with resin
  • can be directly use in resin or plastic
  • simple using and easy storage
  • will not effect the original color
Applications:
  • Engineering plastic including PC, PC/ ABS, ABS, anti dropping
  • Work with GY-FR-OP SERIES, applied on PBT,PET,PA,NYLON flame retard plasic
  • PP?PE?EVA etc. High end flame retard formulation
  • Reach UL94 V-0 with GY-FR-OP SERIES
  • Widely applied on polymers

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 1.85 - 1.89 g/cc
Density 1.86 g/cc
Particle Mesh Size 20 Mesh98% pass
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.10 %
 
Descriptive Properties
AppearanceWhite free flowing powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGOYEN188 / 266496

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.