MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Kazanorgsintez Dust Suppressor "M", Modified Polyethyleneglycolether Mixture
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Production Method: Mixture of polyethylene glycol ethers.

Application: Intended for use as a reactant in the production of potassic fertilizers to decrease dust formation in ore mining plants and to control dustiness of the atmosphere.

Information Provided by Kazanorgsintez

Key Words: PEG
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
pH >= 9.0>= 9.0pH value of water solution with 10% mass fraction
Kinematic Viscosity >= 110 cSt>= 110 cSt
 
Thermal PropertiesMetricEnglishComments
Flash Point >= 130 °C>= 266 °Fin closed cup
 
Component Elements PropertiesMetricEnglishComments
Free Water <= 5.0 %<= 5.0 %
 
Descriptive Properties
AppearanceDark-brown liquid, free from mechanical impurities

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKAZAN159 / 127478

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.