MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

RAMPF RAKU-TOOL® RS-9160 Platinum Silicone
Categories: Polymer; Thermoset; Silicone

Material Notes: 60A Platinum Silicone

Key Properties:

  • High Strength
  • High Durometer
  • Minimal Shrinkage
  • Easy 10:1 Mix
Applications:
  • Room temperature hand batch processing
  • Hobby and arts projects
  • Rapid prototyping rollers
  • Mold making
Cure: 7 days @ 77°F (25°C)

Information provided by © RAMPF Tooling Solutions GmbH & Co. KG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³Activator; ASTM D-792
 1.12 g/cc0.0405 lb/in³ASTM D-792
 1.35 g/cc0.0488 lb/in³Silicone; ASTM D-792
Viscosity 3200 cP3200 cPActivator; ASTM D-2393
 28000 cP28000 cPMixture; ASTM D-2393
 51500 cP51500 cPSilicone; ASTM D-2393
Storage Temperature 15.0 - 30.0 °C59.0 - 86.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 55 - 6555 - 65Cured; ASTM D-2240
Tensile Strength 6.21 MPa900 psiCured; ASTM D-638
Elongation at Break 135 %135 %Cured; ASTM D-638
Tear Strength 24.5 kN/m140 pliCured; ASTM D-624
 
Processing PropertiesMetricEnglishComments
Cure Time 960 - 1440 min16.0 - 24.0 hourDemold
Working Life 50.0 - 85.0 min50.0 - 85.0 min
 
Descriptive Properties
AspectPurpleCure
ColorPurpleActivator
 WhiteSilicone
Mix Ratio100:10Silicone, Weight
 100:13Activator, Volume

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRAMPF191 / 317791

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.