MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

SABIC NORYL™ Resin SE1X Polyphenylene Ether + PS (PPE+PS) (Americas)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL™ SE1X resin is a non-reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This injection moldable grade contains non-brominated, non-chlorinated flame retardant and carries a UL94 flame rating of V0/V1 at 1.5mm along with a UL746C Outdoor Suitability rating of F1. NORYL SE1X resin offers strong electrical performance, low moisture absorption, dimensional stability, and hydrolytic stability. This material is an excellent candidate for indoor and outdoor electrical enclosures , heating ventilation / air conditioning (HVAC) applications, and solar / photovoltaic (PV) junction box applications. *for enhanced processing version, please see NORYL NH5120 resin grade.

Features: Weatherable,Non-Halogenated,Non-Chlorinated,Non-Brominated

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/ccASTM D792
Water Absorption 0.060 %
@Time 86400 sec
0.060 %
@Time 24.0 hour
ASTM D570
Moisture Absorption 0.0200 %0.0200 %Injection Molding
Viscosity 8.0 cP
@Load 5.00 kg,
Temperature 280 °C
8.0 cP
@Load 11.0 lb,
Temperature 536 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0070 in/in
@Thickness 0.126 in
SABIC method
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/inSABIC method
Melt Flow 8.5 g/10 min
@Load 5.00 kg,
Temperature 280 °C
8.5 g/10 min
@Load 11.0 lb,
Temperature 536 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 50.0 MPa7250 psi50 mm/min; ISO 527
 53.0 MPa7690 psi50 mm/min; ASTM D638
Tensile Strength, Yield 61.0 MPa8850 psi50 mm/min; ISO 527
 65.0 MPa9430 psi50 mm/min; ASTM D638
Elongation at Break 15 %15 %50 mm/min; ASTM D638
 20.7 %20.7 %50 mm/min; ISO 527
Elongation at Yield 4.0 %4.0 %50 mm/min; ASTM D638
 4.3 %4.3 %50 mm/min; ISO 527
Tensile Modulus 2.50 GPa363 ksi50 mm/min; ASTM D638
 2.67 GPa387 ksi1 mm/min; ISO 527
Flexural Strength 99.0 MPa14400 psiyield, 2 mm/min; ISO 178
 100 MPa14500 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
 100 MPa14500 psiyld, 2.6 mm/min, 100 mm span; ASTM D790
Flexural Modulus 2.40 GPa348 ksi2.6 mm/min, 100 mm span; ASTM D790
 2.56 GPa371 ksi2 mm/min; ISO 178
 2.70 GPa392 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 180 J133 ft-lbASTM D256
 106 J
@Temperature -30.0 °C
78.2 ft-lb
@Temperature -22.0 °F
ASTM D256
Izod Impact, Unnotched 26.0 J/cm48.7 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 14.0 kJ/m²6.66 ft-lb/in²80*10*4; ISO 180/1A
Dart Drop, Total Energy 49.0 J36.1 ft-lbASTM D3763
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.30e+16 ohm-cm2.30e+16 ohm-cmASTM D257
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohmASTM D257
Dielectric Constant  2.46
@Frequency 1e+6 Hz
2.46
@Frequency 1e+6 Hz
ASTM D150
 2.52
@Frequency 50.0 - 60.0 Hz
2.52
@Frequency 50.0 - 60.0 Hz
ASTM D150
Dielectric Strength 18.1 kV/mm
@Thickness 3.20 mm
460 kV/in
@Thickness 0.126 in
in oil; ASTM D149
Dissipation Factor  0.0021
@Frequency 1e+6 Hz
0.0021
@Frequency 1e+6 Hz
ASTM D150
 0.0034
@Frequency 50.0 - 60.0 Hz
0.0034
@Frequency 50.0 - 60.0 Hz
ASTM D150
Arc Resistance 60 - 120 sec60 - 120 secASTM D495
Comparative Tracking Index 400 - 600 V400 - 600 VUL 746A
Hot Wire Ignition, HWI >= 120 sec
@Thickness >=1.50 mm
>= 120 sec
@Thickness >=0.0591 in
UL 746A
High Amp Arc Ignition, HAI >= 120 arcs
@Thickness >=1.50 mm
>= 120 arcs
@Thickness >=0.0591 in
UL 746A
High Voltage Arc-Tracking Rate, HVTR >= 150 mm/min>= 5.91 in/minUL 746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 80.4 µm/m-°C
@Temperature -40.0 - 40.0 °C
44.7 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
CTE, linear, Transverse to Flow 88.1 µm/m-°C
@Temperature -40.0 - 40.0 °C
48.9 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 129 °C264 °FEdgew 120*10*4 sp=100mm; ISO 75/Be
 126 °C
@Thickness 3.20 mm
259 °F
@Thickness 0.126 in
unannealed; ASTM D648
 126 °C
@Thickness 6.40 mm
259 °F
@Thickness 0.252 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 115 °C239 °FEdgew 120*10*4 sp=100mm; ISO 75/Ae
 112 °C
@Thickness 3.20 mm
234 °F
@Thickness 0.126 in
unannealed; ASTM D648
 118 °C
@Thickness 6.40 mm
244 °F
@Thickness 0.252 in
unannealed; ASTM D648
Vicat Softening Point 132 °C270 °FRate B/50; ISO 306
 135 °C275 °FRate B/120; ISO 306
UL RTI, Electrical 110 °C230 °FUL 746B
UL RTI, Mechanical with Impact 105 °C221 °FUL 746B
UL RTI, Mechanical without Impact 110 °C230 °FUL 746B
Flammability, UL94  V-1
@Thickness >=1.50 mm
V-1
@Thickness >=0.0591 in
UL 94
 V-0
@Thickness >=6.00 mm
V-0
@Thickness >=0.236 in
UL 94
Glow Wire Ignition Temperature  700 °C
@Thickness 1.00 mm
1290 °F
@Thickness 0.0394 in
IEC 60695-2-13
 700 °C
@Thickness 1.50 mm
1290 °F
@Thickness 0.0591 in
IEC 60695-2-13
 725 °C
@Thickness 2.00 mm
1340 °F
@Thickness 0.0787 in
IEC 60695-2-13
 725 °C
@Thickness 3.00 mm
1340 °F
@Thickness 0.118 in
IEC 60695-2-13
Glow Wire Flammability Index  900 °C
@Thickness 1.00 mm
1650 °F
@Thickness 0.0394 in
IEC 60695-2-12
 900 °C
@Thickness 1.50 mm
1650 °F
@Thickness 0.0591 in
IEC 60695-2-12
 960 °C
@Thickness 2.00 mm
1760 °F
@Thickness 0.0787 in
IEC 60695-2-12
 960 °C
@Thickness 3.00 mm
1760 °F
@Thickness 0.118 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 280 - 310 °C536 - 590 °F
Zone 2 260 - 305 °C500 - 581 °F
Zone 3 270 - 310 °C518 - 590 °F
Melt Temperature 280 - 310 °C536 - 590 °FInjection Molding
Mold Temperature 75.0 - 105 °C167 - 221 °F
Drying Temperature 105 - 110 °C221 - 230 °FInjection Molding
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hourInjection Molding
 8.00 hour8.00 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Shot Size 30 - 70 %30 - 70 %
Screw Speed 20 - 100 rpm20 - 100 rpm
 
Descriptive Properties
Radiant Panel ListingRP100UL Tested
UV-light, water exposure/immersionF1UL 746C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82474 / 290421

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.