MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Michelman® CleanGrip® 2100 Silica based, sprayable nonskid coating
Categories: Ceramic; Oxide; Silicon Oxide; Fluid

Material Notes: Description: Water based frictionizing agent

Usage: CleanGrip® 2100 is a silica based, sprayable nonskid coating designed to reduce the slipperiness of shipping containers by providing excellent slide angles. Because CleanGrip® 2100 is easily cleanable, it takes the worry and mess out of running non-skids. This product is gluable using both hot melt and cold set adhesives.

Application data: CleanGrip® 2100 is designed to be applied by spray coater; however, other application methods (such as felts, sponges or rollers) are also possible.

Frequently applied at the paper mill, typical uses include: Corrugated packaging for non-perishables; Folding cartons and Multi-wall bags

Food Contact Information when manufactured in the USA and Belgium:
FDA:
176.170: Components of paper and paperboard in contact with aqueous and fatty foods.
176.180: Components of paper and paperboard in contact with dry foods.

Information provided by Michelman®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.06 - 1.08 g/cc1.06 - 1.08 g/cc
pH 8.78 - 108.78 - 10
Brookfield Viscosity <= 50 cP<= 50 cPSpindle # 1, rpm 60
Viscosity Measurement 12 - 2212 - 22[sec], EZ cup, Cup # 2
 
Descriptive Properties
AppearanceThin, translucent liquid
Solids TypeSilica

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WMICHEL003 / 134920

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.