MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Eastman Eastar GN125 Copolyester, Natural  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Unreinforced

Material Notes: Eastar Copolyester GN125 is a glycol modified polyethylene terephthalate (PET) that contains an ultraviolet light inhibitor. This product is recommended for indoor applications requiring enhanced color stability. Eastar copolyester GN125 will not crystallize and as a result, offers a wider processing latitude than conventional crystallizable polyesters. This product offers an excellent combination of clarity, toughness, and melt strength that makes if useful for a variety of processing techniques and end-use applications.

Applications/Uses

  • Cosmetics/personal care packaging
  • Writing Instruments
  • Point of purchase displays
  • Toys/Sporting goods
  • Lighting

  • Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Specific Gravity 1.30 g/ccASTM D792
    Water Absorption 0.13 %24h Immersion; ASTM D570
    Linear Mold Shrinkage 0.0020 - 0.0050 cm/cm
    @Thickness 3.20 mm
    ASTM D955
     
    Mechanical PropertiesOriginal ValueComments
    Hardness, Rockwell R 106ASTM D785
    Tensile Strength at Break 27.0 MPaISO 527
     30.0 MPaASTM D638
    Tensile Strength, Yield 49.0 MPaASTM D638
     49.0 MPaISO 527
    Elongation at Break 110 %ISO 527
     150 %ASTM D638
    Elongation at Yield 4.0 %ISO 527
     4.3 %ASTM D638
    Tensile Modulus 2.01 GPaASTM D638
     2.02 GPaISO 527
    Flexural Strength 69.0 MPaISO 178
     71.0 MPaASTM D790
    Flexural Modulus 2.10 GPaISO 178
     2.20 GPaASTM D790
    Izod Impact, Notched 0.270 J/cm
    @Temperature -40.0 °C
    ASTM D256
     98.0 J/m
    @Temperature 23.0 °C
    ASTM D256
    Izod Impact, Unnotched NBASTM D4812
     NB
    @Temperature -40.0 °C
    ASTM D4812
    Izod Impact, Notched (ISO) 3.90 kJ/m²
    @Temperature -40.0 °C
    ISO 180
     8.10 kJ/m²
    @Temperature 23.0 °C
    ISO 180
     
    Thermal PropertiesOriginal ValueComments
    Deflection Temperature at 0.46 MPa (66 psi) 69.0 °CISO 75
     69.0 °CASTM D648
    Deflection Temperature at 1.8 MPa (264 psi) 60.0 °CASTM D648
     62.0 °CISO 75
     
    Optical PropertiesOriginal ValueComments
    Haze 0.30 %ASTM D1003
    Transmission, Visible 91 %Total Transmittance; ASTM D1003
     
    Processing PropertiesOriginal ValueComments
    Melt Temperature 249 - 271 °C
    Mold Temperature 16.0 - 38.0 °C
    Drying Temperature 71.0 °C
    Dry Time 4 - 6 hour

    **
    Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

    Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Eastman Eastar GN078 Copolyester, Natural
    Eastman Eastar GN002 Copolyester, Natural
    Eastman Eastar GN005 Copolyester, Natural
    Eastman Eastar GN046 Copolyester, Natural
    Polymer Resources PC-GP1-10TFE Polycarbonate, General Purpose, Wear Resistant, Low Flow

    PE9045 / 35101

    Aluminum Castings

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.