Description: TATREN TPO 12 76 is a controlled rheology extra high impact resistance thermoplastic polyolefin with exceptional impact properties even at low temperatures. It is a grade of medium fluidity. This grade contains nucleating agent. TATREN TPO 12 76 is characterized by exceptionally high impact resistance even at minus temperatures and very good impact/stiffness balance. Applications: TATREN TPO 12 76 is intended especially for compounding and subsequent injection molding of products where excellent impact resistance at minus temperatures is required. This grade is intended to be used in automotive industry. In regard of extra high impact properties of the grade it is very often not necessary to add any rubber modifier for the purpose to increase impact behavior for heavy applications. When used in blends it also allows usage of higher portion of regranulates while there is not deterioration of impact properties, which makes this grade to be economically very attractive raw material. (1) Typical properties measured on standard injection molded test specimen according to ISO 294-1. (2) Values have been measured on standard injected molded specimens prepared in accordance with internal method. Information provided by Molgroup Chemicals |