MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

ExxonMobil Mobil Pyrogard 53
Categories: Fluid; Lubricant

Material Notes: Mobil Pyrogard 53 is a high performance phosphate ester synthetic fluid designed to replace petroleum-based oils in hydraulic applications where operating conditions preclude the use of combustible petroleum products. Mobil Pyrogard 53 is approved by Factory Mutual (FM) as a fire-resistant fluid. Mobil Pyrogard 53 has excellent resistance to oxidation at temperatures normally encountered in hydraulic systems and gives long service life without the formation of deleterious sludges and other materials. It resists foaming and separates readily from water. It offers good antiwear protection for high pressure, high output hydraulic pumps and is very resistant to shear so that it retains its viscosity throughout its service life. The product provides good long-term rust protection, provided there is proper control to avoid excessive water contamination. Mobil Pyrogard 53 has a specific gravity greater than that of water. Any water in the system will float to the top of the reservoir where it can easily be removed. The high specific gravity also affects the flow characteristics of the fluid and must be taken into account in the design and maintenance of the system. The successful experience over the years in a wide variety of hydraulic applications where fire resistance is a key concern has made Mobil Pyrogard 53 the product of choice for many users.

Application considerations: Seal and accumulator bladder materials must be compatible with Mobil Pyrogard 53. Butyl rubber, silicon, Teflon, Viton or equivalent materials are satisfactory. Neoprene and Buna N seals, normally used with petroleum fluids, will swell excessively and will deteriorate. Generally, only seals on moving parts and accumulator bladders need be changed. Seals and gaskets on stationary parts will swell and seal more tightly, so they need not be changed until the next scheduled overhaul of the system. In common with other synthetic fire-resistant fluids of this type, Mobil Pyrogard 53 will soften and loosen paint unless it has been specially selected for compatibility with these fluids. When changing from petroleum oil to a phosphate ester fluid, completely remove the paint from the reservoir and leave the reservoir unpainted. If this is not possible, clean suction screens frequently to prevent pump cavitation or starvation. Water-glycol and emulsion-type fluids are not compatible with Mobil Pyrogard 53. Systems must be thoroughly drained and flushed before installing a new charge of Mobil Pyrogard 53. Mobil Pyrogard 53 is recommended for hydraulic applications where fire resistant type fluids are required. While there may be various possible sources of ignition in many industrial facilities, plants where metals are smelted or hot-worked are perhaps most at risk. Such plants frequently have a history of damage to and leakage from hydraulic system hoses and other components. For safety reasons, Mobil Pyrogard 53 is recommended in these situations. Specific applications include: Aluminium die casting machines; Tilting systems of cast iron induction melting furnaces; Various steel industry applications where fire hazard is a key concern

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.155 g/cc
@Temperature 15.6 °C
1.155 g/cc
@Temperature 60.1 °F
Kinematic Viscosity at 40°C (104°F) 41.8 cSt41.8 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 5.1 cSt5.1 cStASTM D445
 
Thermal PropertiesMetricEnglishComments
Pour Point 0.000 °C32.0 °FASTM D97
Flammability Test 538538Auto Ignition [°C]
Flash Point 246 °C475 °FASTM D92

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum A360.0-F Die Casting Alloy
Aluminum 360.0-F Die Casting Alloy
Overview of materials for Silicone Rubber
Aclo Accutech Polypropylene Copolymer CP0436G10CL Glass Reinforced
Americhem Engineered Compounds ColorFast® ACR100 Polymethylmethacrylate

WEXXON100 / 75525

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.