MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Celanese VECTRA MT1335 LCP, Medical Technology
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP)

Material Notes: Best High Current Arc Ignition (HAI) performance. Glass/PTFE filled.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.62 g/cc0.0585 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0010 cm/cm0.0010 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0040 cm/cm0.0040 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 5555ISO 2039-2
Tensile Strength at Break 171 MPa24800 psi5mm/min; ISO 527-2/1A
Elongation at Break 3.3 %3.3 %5mm/min; ISO 527-2/1A
Tensile Modulus 11.0 GPa1600 ksi50mm/min; ISO 527-2/1A
Flexural Strength 206 MPa29900 psiISO 178
Flexural Modulus 10.5 GPa1520 ksiISO 178
Compressive Strength 77.0 MPa
@Strain 1 %
11200 psi
@Strain 1 %
ISO 604
Compressive Modulus 10.5 GPa1520 ksiISO 604
Izod Impact, Notched (ISO) 17.0 kJ/m²8.09 ft-lb/in²ISO 180/1A
 33.0 kJ/m²
@Temperature 23.0 °C
15.7 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1U
Charpy Impact Unnotched 3.80 J/cm²18.1 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 2.60 J/cm²12.4 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohmIEC 60093
Dielectric Constant  3.1
@Frequency 1e+6 Hz
3.1
@Frequency 1e+6 Hz
IEC 60250
 3.5
@Frequency 100 Hz
3.5
@Frequency 100 Hz
IEC 60250
Dielectric Strength 32.0 kV/mm813 kV/inIEC 60243-1
Dissipation Factor  0.016
@Frequency 1e+6 Hz
0.016
@Frequency 1e+6 Hz
IEC 60250
 0.020
@Frequency 100 Hz
0.020
@Frequency 100 Hz
IEC 60250
Arc Resistance 130 sec130 secInternal
Comparative Tracking Index 175 V175 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Transverse to Flow 19.0 µm/m-°C10.6 µin/in-°FISO 11359-2
Melting Point 280 °C536 °F10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 0.46 MPa (66 psi) 250 °C482 °FISO 75-1, -2
Deflection Temperature at 1.8 MPa (264 psi) 230 °C446 °FISO 75-1, -2
Deflection Temperature at 8.0 MPa 162 °C324 °FISO 75-1, -2
Vicat Softening Point 146 °C295 °FISO 306
Flammability, UL94 V-0V-0
 
Processing PropertiesMetricEnglishComments
Processing Temperature 80.0 - 120 °C176 - 248 °Fcavity
 285 - 295 °C545 - 563 °Fhot runner
Feed Temperature 60.0 - 80.0 °C140 - 176 °F
Zone 1 270 - 280 °C518 - 536 °F
Zone 2 275 - 285 °C527 - 545 °F
Zone 3 280 - 290 °C536 - 554 °F
Zone 4 285 - 295 °C545 - 563 °F
Die Temperature 290 - 300 °C554 - 572 °F
Melt Temperature 285 - 295 °C545 - 563 °F
 293 °C559 °FISO 294
Mold Temperature 60.0 °C140 °FISO 294
Injection Velocity 150 mm/sec5.91 in/secISO 294
Drying Temperature >= 150 °C>= 302 °F
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hour
Moisture Content <= 0.010 %<= 0.010 %
Injection Pressure 50.0 - 150 MPa7250 - 21800 psi
Hold Pressure 48.0 MPa6960 psiISO 294
 50.0 - 150 MPa7250 - 21800 psi
Back Pressure <= 3.00 MPa<= 435 psi
Screw Speed  80 rpm
@Diameter 40.0 mm
80 rpm
@Diameter 1.57 in
 140 rpm
@Diameter 25.0 mm
140 rpm
@Diameter 0.984 in
 200 rpm
@Diameter 16.0 mm
200 rpm
@Diameter 0.630 in
 
Descriptive Properties
Injection moldingYes
Injection speedvery fast

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese VECTRA MT1300 LCP, Medical Technology
Covestro Texin® 5250 Thermoplastic Polyurethane, Polyether-based, Medical
Möller Medical NanoSkin 101 NanoCoating
NuSil MED-166 Silicone, Primer - Unrestricted Medical Use
RTP Company RTP 3400-3 TFE 20 Liquid Crystal Polymer (LCP), PTFE Lubricated

PHCQ521 / 178976

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.