MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
3D Systems Accura® e-Stone™ PEACH Plastic for SLA® Systems
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer

Material Notes: 3D Systems Accura e-Stone PEACH material for SLA is designed to produce durable dental models for individual teeth and arches with crisp resolution, extreme accuracy and repeatability. It has the appearance of traditional dental stone and its high contrast peach color provides improved visualization. Accura e-Stone models are used in digital dentistry workflows for a range of dental applications, including drilling, grinding and waxing.

Applications:

  • Replacement for dental stone
  • Crown and bridge restorations
  • Orthodontic working and study models
  • Orthodontic thermoforming applications
Benefits:
  • Compatible with standard dental lab practices
  • Reduce breakage vs. plaster
  • Decreased steps vs. impression based systems
  • Increased visual detail for better margin viewing
  • Reproducible and archivable for easy remakes
Features:
  • Durable
  • Accurate
  • High contrast peach color
  • Digital production

Information provided by 3D Systems

Vendors:
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.13 g/ccLiquid
 1.19 g/ccSolid
Viscosity 200 - 300 cP
@Temperature 30.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 80Large Frame SLA Printers
 80Projet SLA Printers
Tensile Strength 37.0 - 39.0 MPaLarge Frame SLA Printers; ASTM D 638
 38.0 MPaProjet SLA Printers; ASTM D 638
Elongation at Break 10 - 23 %Large Frame SLA Printers; ASTM D 638
 17 %Projet SLA Printers; ASTM D 638
Tensile Modulus 1500 - 1750 MPaLarge Frame SLA Printers; ASTM D 638
 1630 MPaProjet SLA Printers; ASTM D 638
Flexural Strength 54.0 - 59.0 MPaLarge Frame SLA Printers; ASTM D 790
 57.0 MPaProjet SLA Printers; ASTM D 790
Flexural Modulus 1350 - 1750 MPaLarge Frame SLA Printers; ASTM D 790
 1550 MPaProjet SLA Printers; ASTM D 790
Izod Impact, Notched 18.0 - 25.0 J/mLarge Frame SLA Printers; ASTM D 256
 22.0 J/mProjet SLA Printers; ASTM D 256
Penetration 4.2[mils]
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 58.0 - 63.0 °CLarge Frame SLA Printers; ASTM D 648
 61.0 °CProjet SLA Printers; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 51.0 - 55.0 °CLarge Frame SLA Printers; ASTM D 648
 53.0 °CProjet SLA Printers; ASTM D 648
Glass Transition Temp, Tg 60.0 °CLarge Frame SLA Printers
 60.0 °CProjet SLA Printers
 
Descriptive Properties
ColorPeach
Critical Exposure (Ec)10.5 mJ/cm3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAPPR3105 / 239073

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.