MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
CHT Group QSil 568 Addition Cure Potting Material
Categories: Polymer; Thermoset; Silicone

Material Notes: Product Description: QSil 568 is a 100% silicone semi-thixotropic compound designed for potting and encapsulation applications.

Key Features:

  • 100% solids
  • One hour gel time
  • Semi-thixotropic
  • Heat cure required

Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.980 g/ccUncatalyzed, QSil 568B
 1.48 g/ccUncatalyzed, QSil 568A
Viscosity 3000 cPUncatalyzed, QSil 568B
 80000 cPUncatalyzed, QSil 568A
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 50Cure 17 minutes at 150°C
Tensile Strength 450 psiCure 17 minutes at 150°C
Elongation at Break 200 %Cure 17 minutes at 150°C
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 6.02e+15 ohm-cm
Dielectric Constant 3.27
@Frequency 1000 Hz
Dielectric Strength 22.6 kV/mm
Dissipation Factor 0.0090
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 204 °C
Minimum Service Temperature, Air -55.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 17.0 min
@Temperature 150 °C
As Tested
Gel Time 60.0 minCatalyzed
 
Descriptive Properties
ColorBlackUncatalyzed, QSil 568B
 WhiteUncatalyzed, QSil 568A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PACC2103 / 199491

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.