MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Ensinger TECANYL® black Polyphenylene oxide
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO

Material Notes:
  • electrically insulating
  • high strength
  • good dimensional stability
  • high toughness
  • high thermal resistance
Target Industries:
  • conveyor technology
  • mechanical engineering
  • food processing
  • precision engineering
  • automotive industry
  • electrical engineering
  • home appliances
Noryl EN 265

Information provided by Ensinger Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.08 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 119ASTM D 785
Tensile Strength at Break 9200 psiASTM D 638
Tensile Strength, Yield 9000 psiASTM D 638
Elongation at Break 25 %ASTM D 638
Modulus of Elasticity 350 ksiASTM D 638
Flexural Strength 13400 psiASTM D 790
Flexural Modulus 370000 psiASTM D 790
Izod Impact, Unnotched 3.50 ft-lb/inASTM D 256
Coefficient of Friction, Dynamic 0.39
@Pressure 0.276 MPa
50 fpm; ASTM D 3702
Coefficient of Friction, Static 0.32ASTM D 3702
 
Thermal PropertiesOriginal ValueComments
CTE, linear 33.0 µin/in-°FASTM D 696
Maximum Service Temperature, Air 254 °FLong Term
 279 °FIntermittent
Deflection Temperature at 0.46 MPa (66 psi) 279 °FASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 254 °FASTM D 648
Vicat Softening Point 310 °F
Flammability, UL94 V-1
@Thickness 1.50 mm
 V-0
@Thickness 6.00 mm
 
Descriptive Properties
Colorblack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PENSIN8178 / 319106

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.