MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Multibase Multi-Flex® D 3104 TPO Thermoplastic Polyolefin Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyolefin

Material Notes:

Features:

  • Chemical Resistance, Good
  • Paintable
  • Ozone Resistant
  • Thermal Stability, Good
  • Density, Low
  • Tear Strength, Good
  • Forms:

  • Pellets
  • Processing Method:

  • Injection Molding
  • Uses:

  • Automotive Applications
  • Information provided by Multibase

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Specific Gravity 0.902 g/ccASTM 792
    Linear Mold Shrinkage 0.012 cm/cmASTM D955
    Melt Flow 3.0 g/10 min
    @Load 2.16 kg,
    Temperature 230 °C
    ASTM D1238
     
    Mechanical PropertiesOriginal ValueComments
    Hardness, Shore D 3910 seconds; ASTM D2240
    Tensile Strength, Yield 2300 psiElastic; ASTM D412
    Elongation at Break 540 %Elastic; ASTM D412
    Flexural Modulus 28000 psiASTM D790
    Tear Strength 480 pliASTM D624
     
    Processing PropertiesOriginal ValueComments
    Rear Barrel Temperature 350 - 390 °F
    Middle Barrel Temperature 390 - 430 °F
    Front Barrel Temperature 430 - 450 °F
    Nozzle Temperature 430 - 450 °F
    Melt Temperature 450 °F
    Mold Temperature 100 °F
     
    Descriptive Properties
    Clamp Tonnage2-4 tons/in2
    Screw L/D Ratio20:1

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Multibase Multi-Flex® D 5304 Black TPO Thermoplastic Polyolefin Elastomer
    Multibase Multi-Flex® D 5308 848 Black TPO Thermoplastic Polyolefin Elastomer
    Multibase Multi-Flex® D 5308 Platinum TPO Thermoplastic Polyolefin Elastomer
    Multibase Multi-Flex® D 5500 TPO Thermoplastic Polyolefin Elastomer
    Multibase Multi-Flex® A 6221 CUV A VY Dk Pewter TPO Thermoplastic Polyolefin Elastomer

    PMULTI099 / 54003

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.