MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
CHT CHT-BeauSil™ AMO 8950 EM Amodimethicones
Categories: Other Engineering Material

Material Notes: Description: Amodimethicones are functionalized silicones with nitrogen groups. These modification improves the deposite and the affinity to the hair. Amodimethicones are showing excellent combing and a good gloss on hair. These silicone polymers are ideal for all kind of hair care application were best performance is needed.

Key Features

  • Improves dry and wet combing
  • Color and heat protection
  • Softness
  • Conditioning
Key Applications
  • Conditioner
  • Shampoo
  • Hair Treatment
Application: CHT-BeauSil™ AMO 8950 EM is a 50% solids cationic emulsion of an amine-functional silicone polymer. The amodimethicone actives are delivered in an opaque, low viscosity liquid with a neutral pH. This emulsion was developed as a conditioning additive for hair care products such as shampoos, conditioners, styling aids, and hair colorants. This product has an industry leading particle size resulting in increased stability and performance.

Addition Rates
Dosage – 1: 0.5-5.0% in Shampoos
Dosage - 2: 1.0 - 5.0% in Conditioners
Dosage - 3: 0.1 - 0.3% in Leave-On products

INCI Name: Amodimethicone (and) Trideceth-12 (and) Cetrimonium Chloride

Information provided by CHT Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles 50 %
Storage Temperature 4.00 - 40.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Descriptive Properties
AppearanceWhite emulsion
IonicityCationic
MIT FreeYes
Ultralow cyclic contentNo

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHTSIL292 / 314775

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.