MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

PSM Industries Pacific Sintered Metals FN-253-S(HT) 4600 Powdered Metal (MPIF FL-4605-100HT)
Categories: Metal; Ferrous Metal

Material Notes: High performance material with high strength and wear resistance after heat treatment.

Equivalent MPIF Specification: FL-4605-100HT

All information provided by Pacific Sintered Metals.

Key Words: PM
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 6.80 - 7.20 g/cc0.246 - 0.260 lb/inĀ³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 2929
Tensile Strength, Ultimate 689 MPa100000 psi
Tensile Strength, Yield 689 MPa100000 psi
Elongation at Break <= 0.50 %<= 0.50 %
Modulus of Elasticity 124 GPa18000 ksi
Flexural Strength 1140 MPa165000 psiTransverse Rupture
Charpy Impact, Unnotched 6.10 J4.50 ft-lb

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for High Carbon Steel
PSM Industries Pacific Sintered Metals FN-253-T(HT) 4600 Powdered Metal (MPIF FL-4605-140HT)
Overview of materials for Cold Work Steel
PSM Industries Pacific Sintered Metals FCC-216-P(HT) High Carbon Copper Steel Powdered Metal (MPIF FC-0208-50HT)
PSM Industries Pacific Sintered Metals FX-232-T(HT) Infiltrated High Carbon Steel Powdered Metal (MPIF FX-1008-110HT)

NPACIF022 / 86180

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.