MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC GELOY™ XTPMFR10 ASA (Asia)
Categories: Polymer; Thermoplastic; ASA Polymer

Material Notes: PC/ASA, chlorine and bromine free.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.18 g/cc0.0426 lb/in³ISO 1183
Viscosity 105 cP
@Shear Rate 1500 1/s,
Temperature 260 °C
105 cP
@Shear Rate 1500 1/s,
Temperature 500 °F
melt; ISO 11443
Melt Flow 30 g/10 min
@Load 2.16 kg,
Temperature 260 °C
30 g/10 min
@Load 4.76 lb,
Temperature 500 °F
cm³/10 min; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 46.0 MPa6670 psi5 mm/min; ISO 527
 47.0 MPa6820 psi50 mm/min; ASTM D638
 47.0 MPa6820 psi50 mm/min; ISO 527
 49.0 MPa7110 psi5 mm/min; ASTM D638
Tensile Strength, Yield 60.0 MPa8700 psi5 mm/min; ASTM D638
 61.0 MPa8850 psi5 mm/min; ISO 527
 65.0 MPa9430 psi50 mm/min; ASTM D638
 66.0 MPa9570 psi50 mm/min; ISO 527
Elongation at Break 21 %21 %50 mm/min; ISO 527
 31 %31 %50 mm/min; ASTM D638
 50 %50 %5 mm/min; ISO 527
 58 %58 %5 mm/min; ASTM D638
Elongation at Yield 4.0 %4.0 %5 mm/min; ISO 527
 4.0 %4.0 %5 mm/min; ASTM D638
 4.0 %4.0 %50 mm/min; ISO 527
 4.0 %4.0 %50 mm/min; ASTM D638
Tensile Modulus 2.68 GPa389 ksi50 mm/min; ASTM D638
 2.68 GPa389 ksi1mm/min; ISO 527
Flexural Yield Strength 97.0 MPa14100 psi2 mm/min; ISO 178
Flexural Modulus 2.72 GPa395 ksi2 mm/min; ISO 178
Izod Impact, Notched 3.30 J/cm6.18 ft-lb/inASTM D256
 0.900 J/cm
@Temperature -30.0 °C
1.69 ft-lb/in
@Temperature -22.0 °F
ASTM D256
Izod Impact, Notched (ISO) 13.0 kJ/m²6.19 ft-lb/in²80*10*4; ISO 180/1A
 12.0 kJ/m²
@Temperature 0.000 °C
5.71 ft-lb/in²
@Temperature 32.0 °F
80*10*4; ISO 180/1A
Charpy Impact, Notched 1.30 J/cm²6.19 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eA
Impact Test 85.0 J62.7 ft-lbMultiaxial Impact; ISO 6603
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 63.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
35.0 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 63.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
35.0 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C194 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C178 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
Vicat Softening Point 96.0 °C205 °FRate B/50; ISO 306
 98.0 °C208 °FRate B/120; ISO 306
Flammability, UL94 V-0
@Thickness 1.00 mm
V-0
@Thickness 0.0394 in
UL 94 by SABIC-IP
 
Processing PropertiesMetricEnglishComments
Processing Temperature 60.0 - 80.0 °C140 - 176 °FHopper Temperature
Nozzle Temperature 220 - 260 °C428 - 500 °FInjection Molding
Zone 1 200 - 230 °C392 - 446 °F
Zone 2 220 - 260 °C428 - 500 °F
Zone 3 230 - 270 °C446 - 518 °F
Melt Temperature 230 - 270 °C446 - 518 °F
Mold Temperature 50.0 - 70.0 °C122 - 158 °F
Drying Temperature 80.0 - 90.0 °C176 - 194 °FInjection Molding
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourInjection Molding
Moisture Content 0.020 %0.020 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABI10161 / 243628

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.