Key Features:- Toughened system
- Low viscosity and long working life
- Outstanding electrical insulation properties
- Very resistant to thermal cycling and shock
Master Bond EP110F8-3 is a two component high performance epoxy resin system with a long pot life (at least 2-3 days at room temperature). It is used primarily for potting, sealing, encapsulating and casting. This low viscosity system has a convenient and very forgiving one to two mix ratio by weight. It requires an elevated temperature cure at 250-300°F. A typical cure schedule would be 4-6 hours at 250-300°F. For optimum properties, a post cure of 3-5 hours at 350°F is recommended. Even without the optional post cure, EP110F8-3 will perform very well. EP110F8-3 has no solvents or diluents and has low shrinkage upon cure. It adheres well to a wide variety of substrates, including metals, composites, glass and many plastics. It has superior electrical insulation properties. Its physical strength properties of low tensile strength, lower modulus and relatively higher elongation, translates into a special capability to resist severe thermal cycling and shock. It has good resistance to water, oils and fuels. The color of Part A is clear while the color of Part B is amber. The service temperature range is -100°F to +300°F. It can be used in applications where very high performance electrical insulation properties and resistance to rigorous thermal cycling is needed. Product Advantages: - Low viscosity liquid; flows easily
- Long working life at room temperature
- Outstanding thermal shock resistance
- Very high elongation
- Unsurpassed electrical insulation properties
Information provided by Masterbond. |
Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.Click here to view all available suppliers for this material. Please click here if you are a supplier and would like information on how to add your listing to this material. |