MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Celanese Hostaform® CF802 10/9022 POM, Specialty
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM)

Material Notes: Hostaform« acetal copolymer grade CF802 10/9022 is a conductive, fuel compatible general purpose acetal copolymer. Hostaform« CF802 10/9022 has been developed to dissipate static electricity from fuel handling systems. Hostaform« CF802 10/9022 has been specially formulated for laser welding applications.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.47 g/cc0.0531 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 62.0 MPa8990 psi50mm/min; ISO 527-2/1A
Elongation at Yield 10 %10 %50mm/min; ISO 527-2/1A
Tensile Modulus 3.00 GPa435 ksi50mm/min; ISO 527-2/1A
Charpy Impact, Notched 0.400 J/cm²1.90 ft-lb/in²ISO 179/1eA
Tensile Creep Modulus, 1 hour 2130 MPa309000 psiISO 899-1
Tensile Creep Modulus, 1000 hours 1050 MPa152000 psiISO 899-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 300 ohm-cm300 ohm-cmIEC 60093
Surface Resistance 2000 ohm2000 ohmIEC 60093
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 100 µm/m-°C55.6 µin/in-°FISO 11359-2
CTE, linear, Transverse to Flow 120 µm/m-°C66.7 µin/in-°FISO 11359-2
Melting Point 167 °C333 °F10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 1.8 MPa (264 psi) 100 °C212 °FISO 75-1, -2
 
Processing PropertiesMetricEnglishComments
Processing Temperature 80.0 - 120 °C176 - 248 °Fcavity
 190 - 200 °C374 - 392 °Fhot runner
Zone 1 170 - 180 °C338 - 356 °F
Zone 2 175 - 185 °C347 - 365 °F
Zone 3 180 - 190 °C356 - 374 °F
Zone 4 185 - 195 °C365 - 383 °F
Die Temperature 190 - 200 °C374 - 392 °F
Melt Temperature 180 - 200 °C356 - 392 °F
Drying Temperature 80.0 - 100 °C176 - 212 °F
Dry Time 3.00 hour3.00 hour
Injection Pressure 60.0 - 120 MPa8700 - 17400 psi
Hold Pressure 60.0 - 120 MPa8700 - 17400 psi
Back Pressure <= 2.00 MPa<= 290 psi
 
Descriptive Properties
Injection moldingYes
Injection speedslow
Processing conditions acc. ISO9988-2
Screw Speedslow
 slow
 slow
 slow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company RTP 885 Acetal (POM), Carbon Fiber
Celanese Hostaform® XGC25-LW01 POM, 25% Glass Reinforced
Celanese Hostaform® HS15 POM, Unfilled
Celanese Hostaform® EC270TX POM, Specialty
Celanese Hostaform® EC140XF POM, Specialty

PHCQ372 / 178827

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.