Characteristics: Impact Modified: Excellent Electrical Properties, High Heat Resistance Applications: Automotive (Under Hood), Appliances, Casings and Housings Processing: Injection Molding (Melt Temperature: 495-530°F, Mold Temperature: 195-250°F) Petlon® is manufactured by Albis Plastics Corporation and is a registered trademark of Bayer Corporation. As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This product was discontinued prior to the separation. |