MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Akrochem Antioxidant 405
Categories: Other Engineering Material

Material Notes: Product Description: Akrochem Antioxidant 405 is a diphenylamine antidegradant offering excellent heat and oxidation resistance to most natural and synthetic polymers. Its low volatility is better than competitive antioxidants. It has been found using 405 in combination with Akrochem Antioxidant 58 or 60, a synergism produces outstanding heat resistance that is often used in HNBR. Non-blooming at normal loadings of 1 to 4 phr. Like other amine antioxidants, Antioxidant 405 will discolor but only very slightly. Antioxidant 405 typically can be used in most colors except very light whites or yellows. Has wide FDA acceptability where high temperature antioxidants may be needed in a food contact situation. Minimal peroxide interference; no known blooming with recommended usage levels; no effect on cure rates of sulfur cures. Relatively low melt point means exceptionally good dispersion is easy to achieve.

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.14 g/cc
 
Thermal PropertiesOriginal ValueComments
Melting Point 100 °C
 
Descriptive Properties
AppearanceLight Tan Powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAKZCH525 / 315443

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.