MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

A. Schulman BMC T9 General Purpose Molding Compound
Categories: Polymer; Thermoset; Polyester, TS; Polyester (Thermoset) - Rigid

Material Notes: BMC T9 is a low cost, general purpose bulk molding compound designed for the electrical industry. It is UL listed and is used extensively in the manufacture of residential circuit breakers. BMC T9 can be compression, transfer or injection molded. Other applications re bobbins and electrical connectors.

Information provided by Bulk Molding Compounds, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.96 - 2.16 g/cc0.0708 - 0.0780 lb/in³Molded
Linear Mold Shrinkage 0.0020 - 0.0038 cm/cm0.0020 - 0.0038 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Barcol 30 - 5030 - 50
Tensile Strength 48.3 - 62.1 MPa7000 - 9000 psi
Flexural Strength 110 - 138 MPa16000 - 20000 psi
Flexural Modulus 8.27 - 9.65 GPa1200 - 1400 ksi
Compressive Strength 131 - 159 MPa19000 - 23000 psi
Izod Impact, Notched 2.67 - 3.74 J/cm5.00 - 7.00 ft-lb/in
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 13.8 - 15.7 kV/mm350 - 400 kV/inshort time
Arc Resistance >= 180 sec>= 180 sec
Comparative Tracking Index >= 500 V>= 500 V
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C>= 500 °F
Flammability, UL94 HBHB
 
Processing PropertiesMetricEnglishComments
Processing Temperature 138 - 166 °C280 - 330 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
G-10 Fiberglass Epoxy Laminate Sheet
A. Schulman BMC 685 Mineral Filled, Glass Fiber Reinforced Polyester Compound
A. Schulman BMC 695 Vinyl Ester Molding Compound
Westlake EM1550AA Low Density Polyethylene
A. Schulman BMC 6605A Polyester Molding Compound

PBMC913 / 123377

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.