MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Elkem (Bluestar Silicones) Silbione™ TCS 7772 A/B Silicone Polyaddition for Technical Textiles
Categories: Polymer; Thermoset; Silicone

Material Notes: Applications: Thick Coatings/Bonding Materials

Information provided by Elkem Silicones.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.06 g/cc0.0383 lb/in³
Viscosity 200000 cP200000 cP
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 2020
Tensile Strength 4.00 MPa580 psi
Elongation at Break 575 %575 %
Tear Strength 14.0 kN/m80.0 pli
 
Descriptive Properties
Cured ColorTranslucent
Mix Ratio (A:B)1:1
Most Suitable Coating ProcessNozzle Extrusion, Screen Printing
Typical ApplicationsAnti-slip and skin contact compliant
Typical Substrate(s)Nylon, Polyester, Lycra, Blends

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polychloroprene Rubber (CR)
Overview of materials for Nylon 6, Carbon Fiber Filled
Hippe PA 11 Nylon 11
DuPont Mobility and Materials Neoprene AC MEDIUM Polychloroprene Rubber
Cos40 Cork/Neoprene Rubber Sheet

PBLUST214 / 234762

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.