MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Mar-Bal AltraSet MB3000-15NY Thermoset Polyester - Non-Yellowing Grade
Categories: Polymer; Thermoset; Polyester, TS; Thermoset Polyester Glass Filled BMC

Material Notes: MB3000-15NY is a superior chemical-resistant material with excellent flame and track resistance.

Key features include Non-yellowing as well as rated UL 94 5VA @1.5mm. This material is also UL f1 rated. UL file number E80533

Information provided by Mar-Bal, Inc.

Vendors: Mar-Bal is the leading integrated compounder and molder of BMC Thermoset composite products and value added finishing services. Call 440-543-7526 or visit Mar-Bal.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.85 - 1.95 g/cc0.0668 - 0.0704 lb/in³ASTM D792
Water Absorption 0.12 %0.12 %ASTM D570
Linear Mold Shrinkage 0.0050 - 0.015 cm/cm0.0050 - 0.015 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Barcol 45 - 5545 - 55ASTM D2583
Tensile Strength 34.5 - 41.4 MPa5000 - 6000 psiASTM D638
Flexural Strength 124 - 145 MPa18000 - 21000 psiASTM D790
Flexural Modulus 12.4 - 13.1 GPa1800 - 1900 ksiASTM D790
Compressive Strength 96.5 - 110 MPa14000 - 16000 psiASTM D695
Shear Strength 55.2 - 62.1 MPa8000 - 9000 psiASTM D732
Izod Impact, Notched 4.27 - 5.34 J/cm8.00 - 10.0 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength >= 14.2 kV/mm>= 360 kV/inASTM D149
Arc Resistance >= 185 sec>= 185 secASTM D495
Track Resistance >= 60000 sec>= 60000 secInclined-Plane Tracking; ASTM D2303-85
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C>= 500 °FASTM D648
UL RTI, Electrical 130 °C266 °FUL746B
UL RTI, Mechanical with Impact 130 °C266 °FUL746B
UL RTI, Mechanical without Impact 130 °C266 °FUL746B
Flammability, UL94 5VA
@Thickness 1.50 mm
5VA
@Thickness 0.0591 in
Flame Spread Index 1010Class A - Steiner Tunnel Test; ASTM E84
Smoke Density 170170Class A - Steiner Tunnel Test; ASTM E84
 
Descriptive Properties
Color Change - Bisque1-1.5 Delta-Eunder 300°F for 300 hr.
Color Change - White1.2-1.7 Delta-Eunder 300°F for 300 hr.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mar-Bal MB2000-15 Thermoset Polyester Composite Molding Compound
Mar-Bal MB2000-10 Thermoset Polyester Composite Molding Compound
Mar-Bal MB1000-PC Thermoset Polyester Composite Molding Compound
Mar-Bal MB1000-25 Thermoset Polyester Composite Molding Compound
Mar-Bal MB1000-15 Thermoset Polyester Composite Molding Compound

PMARB858 / 233841

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.