MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Mallard Creek Polymers Rovene® 6005 Acrylic Emulsion
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: ROVENE® 6005 is a very soft acrylic, high molecular weight latex emulsion specifically designed for formulation of permanent label adhesives. Its high molecular weight allows the formulation of permanent label adhesives which are high in peel and tack, yet require a minimum amount of tackifier. It was designed to give excellent performance and compatibility with a wide variety of dispersed tackifiers.
APPLICATIONS: ROVENE® 6005 is recommended for pressure sensitive permanent label adhesives.

Information provided by Mallard Creek Polymers

Key Words: latex; adhesive
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 55 - 57 %
Particle Size 0.25 µm
pH 6.5 - 7.0
Brookfield Viscosity 100 - 600 cP#2/20 rpm
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg -38.0 °C
 
Descriptive Properties
EmulsifiersAnionic
Residual Monomer0.04% Max

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMCP004 / 104661

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.