MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Evonik ROHAMERE® 6965-O Methoxypolyethylene Glycol 5000 Methacrylate  (discontinued **)
Categories: Fluid

Material Notes: Application: Water-based coatings, polymerizable emulsifier, textile and water treatment, paper production, additive for concrete.

Appearance: At room temperature, clear colorless to yellowish liquid

Odor: Faintly ester-like

CAS: 26915-72-0

Information Provided by Evonik CYRO. The former Evonik Methacrylates business has been sold to Röhm GmbH, although this trade name was disontinued prior to the sale.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.08 g/cc
Viscosity 90 cP
@Temperature 30.0 °C
 115 cP
@Temperature 25.0 °C
 125 cP
@Temperature 23.0 °C
 145 cP
@Temperature 20.0 °C
 180 cP
@Temperature 15.0 °C
Molecular Weight 5000 g/mol
 
Chemical PropertiesOriginal ValueComments
Acid Value 20[mg KOH/g]; Rohm Method: M4 (acid-base titr., MAAC)
 
Thermal PropertiesOriginal ValueComments
Boiling Point 100 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.408
@Temperature 20.0 °C
 
Component Elements PropertiesOriginal ValueComments
H2O, Water 48 - 52 %Rohm Method: M3 (according to K. Fischer)
 
Descriptive Properties
Degree of Conversion> 95 mol. -%Rohm Method: M94 (NMR)
MEHQ180-220ppm, Rohm Method: M1-1 (HPLC), MEHQ
Solidification Point (°C)<10

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kennametal Stellite Stellite® 33
Crucible Steel AISI 4340 Alloy Steel
AISI 4340 Steel, oil quenched 845°C, 425°C (800°F) temper
AISI 4130 Steel, water quenched 855°C (1570°F), 595°C (1100°F) temper, 100 mm (4 in.) round

PCYR00096 / 101085

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.