MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Chromium Copper, UNS C18500
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Good to excellent corrosion resistance. Excellent cold workability; good hot workability.

Applications: resistance welding electrodes, seam welding wheels, switch gear, electrode holder jaws, cable connectors, current carrying arms and shafts, circuit breaker parts, molds, spot welding tips, flash welding electrodes, electrical and thermal conductors requiring strength, switch contacts.

Available as flat products, wire, rod, tube, and shapes.

UNS C18500 is inactive per the Copper Development Association. UNS C18200, UNS C18400, and UNS C18500 have similar compositions and mechanical properties.

Key Words: CDA 185, CA185
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.89 g/cc0.321 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 234 - 593 MPa33900 - 86000 psi
Tensile Strength, Yield 97.0 - 531 MPa14100 - 77000 psiDepending on temper
Elongation at Break 40 %40 %in 127 mm (2in.).
Modulus of Elasticity 130 GPa18900 ksi
Poissons Ratio 0.300.30Calculated
Machinability 20 %20 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 50.0 GPa7250 ksi
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.6 µm/m-°C
@Temperature 20.0 - 100 °C
9.78 µin/in-°F
@Temperature 68.0 - 212 °F
Thermal Conductivity  171 W/m-K
@Temperature 20.0 °C
1190 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
TB00 temper
 324 W/m-K
@Temperature 20.0 °C
2250 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
TH04 temper
Melting Point 1070 - 1075 °C1960 - 1967 °F
Solidus 1070 °C1960 °F
Liquidus 1075 °C1967 °F
 
Component Elements PropertiesMetricEnglishComments
Chromium, Cr 0.40 - 1.0 %0.40 - 1.0 %
Copper, Cu 99.3 %99.3 %
Lead, Pb <= 0.015 %<= 0.015 %
Lithium, Li <= 0.040 %<= 0.040 %
Phosphorus, P <= 0.040 %<= 0.040 %
Silver, Ag 0.080 - 0.12 %0.080 - 0.12 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chromium Copper, UNS C18400
Chromium Copper, UNS C18200, TB00 Temper flat products
Copper, Cu; Annealed
Extra-high-leaded brass, UNS C35600
Chromium Copper, UNS C18200, TF00 Temper 50 mm Plate

MC18500b1 / 10791

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.