WESTLAKE HIFOR Xtreme SC74853 polymer is a high strength linear low density polyethylene designed for blown film extrusion that contains no slip, high antiblock and processing aid. Films produced with this resin exhibit excellent toughness. Other features of this resin include good impact strength and good machine direction tear resistance.Application/Uses- Fresh produce packaging
FDA: This material complies with FDA regulations in 21 CFR, section 177.1520. Kosher Compliant.All information provided by Westlake Chemical |
Excellent toughness, good impact strength and good machine direction tear resistance |