MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger TECATEC PEEK GF50 CP/IP/OS S0001 natural Polyetheretherketone, Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Glass Fiber Filled

Material Notes: Fillers: glass fibers

Main features:

  • electrically insulating
  • inherent flame resistance
  • very good mechanical strength
Target Industries:
  • automotive industry
  • aircraft and aerospace technology
  • mechanical engineering
  • oil and gas industry
  • safety engineering
  • sporting goods

Information provided by Ensinger Composites.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.90 g/cc0.0686 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 450 MPa65300 psiISO 527-4
Tensile Modulus 24.0 GPa3480 ksiISO 527-4
Flexural Strength 445 MPa64500 psiISO 14125
Flexural Modulus 22.0 GPa3190 ksiISO 14125
Shear Strength 41.0 MPa5950 psiinterlaminar; ISO 14130
 105 MPa15200 psiinterplanar; ISO 14129
 
Thermal PropertiesMetricEnglishComments
CTE, linear 10.0 µm/m-°C5.56 µin/in-°Fin 0° and 90° direction
Melting Point 343 °C649 °F
Maximum Service Temperature, Air 260 °C500 °Flong term
 300 °C572 °Fshort term
Glass Transition Temp, Tg 143 °C289 °F
 
Processing PropertiesMetricEnglishComments
Drying Temperature 150 °C302 °F
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hour
 
Descriptive Properties
Areal weight finished product455 g/m²
Colornatural
Fiber architectureUS 7781
Fiber areal weight296 g/m²
Fiber typeE glass
Fiber volume content0.5
Material widths1000 mm
 1270 mm
ply thickness (consolidated)0.21 mm
Resin weight content0.349

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENSIN521 / 287745

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.