MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC SABIC® LDPE 2102N3W PE (Global)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: SABIC® LDPE 2102N3W is a general purpose grade with a high level of anti block and slip agent. This grade offers good optical properties and a very good draw down ability. Application SABIC® LDPE 2102N3W is typically used for packaging films for food and industrial goods and for lamination films. This grade is typically used when high draw down is required The usual melt-2 film thickness can be reduced by 10-40%, maintaining an adequate CoF level. SABIC® LDPE 2102N3W can typically be used for food applications due to very low migration levels. Film properties Film properties have been measured at film of 25 µm with a BUR of 3. The film has been produced on Kiefel IBC blown film line with 200 kg/h. Die size 200 mm, die gap 0.8 mm. This product is not intended for and must not be used in any pharmaceutical/medical applications.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.921 g/cc0.0333 lb/in³ASTM D1505
Melt Flow 2.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.5 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 13.0 MPa1890 psiISO 527-3
Film Tensile Strength at Yield, TD 11.0 MPa1600 psiISO 527-3
Film Elongation at Break, MD >= 100 %>= 100 %ISO 527-3
Film Elongation at Break, TD >= 500 %>= 500 %ISO 527-3
Tensile Modulus 0.190 GPa27.6 ksiTD; ISO 527-3
Coefficient of Friction 0.200.20ASTM D1894
Tear Strength 20.0 kN/m114 pliTD; ISO 6383-2
 50.0 kN/m285 pliMD; ISO 6383-2
Dart Drop Total Energy 200 J/cm0.375 ft-lb/milASTM D4272
Film Tensile Strength at Break, MD 30.0 MPa4350 psiISO 527-3
Film Tensile Strength at Break, TD 18.0 MPa2610 psiISO 527-3
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 90.0 °C194 °Fat 10 N (VST/A); ISO 306
 
Optical PropertiesMetricEnglishComments
Haze 12 %12 %ASTM D1003
 
Descriptive Properties
Blocking<5 gSABIC method
Clarity30 mVSABIC method
Re-blocking10 gSABIC method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABI10958 / 244425

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.