MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Renegade Materials Corporation RM-5001 Cyanate Ester Prepreg, 3K 8HS Fabric
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset

Material Notes: RM-5001 cyanate ester is a very low outgassing, toughened, high performance prepreg.

  • Straightforward 350°F Cure
  • Designed for the unique requirements of satellite and missile structures
  • Low shrinkage during cure
  • Developed for consistent handling and superior performance
  • Continuous service up to and including 350F with post cure
  • Available in woven and unidirectional product forms using all fibers including carbon, quartz and S2 glass
  • Nano-enhancement for tailored laminate properties and multi-functional performance
  • Low moisture absorption

    Information provided by Renegade Materials Corporation.

    Renegade Materials has been acquired by Teijin.

  • Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Density 1.19 g/ccResin
    Moisture Absorption at Equilibrium 1.1 %Post cured at 350°F
     1.2 %Post cured at 450°F
     
    Mechanical PropertiesOriginal ValueComments
    Elongation at Break 4.0 %Resin
    Flexural Strength 14.6 ksiResin, RT, Wet
     15.0 ksiResin, RT, Dry
     155.1 ksiPrepreg, Warp Direction, RT, Dry, Normalized to 60% fiber volume fraction; ASTM D7264
    Flexural Modulus 460 ksiResin, RT, Dry; ASTM D6272
     460 ksiResin, RT, Wet
     10800 ksiPrepreg, Warp Direction, RT, Dry; ASTM D7264
    Compressive Strength 115 ksiPrepreg, Warp Direction, RT, Dry; ASTM D6641
    Compressive Modulus 9.50e+6 psiPrepreg, Warp Direction, RT, Dry; ASTM D6641
    Shear Strength 8.10 ksiIn-Plane, RT, Dry; ASTM D3518
     10.4 ksiInterlaminar, RT, Dry; ASTM D2344
     
    Electrical PropertiesOriginal ValueComments
    Dielectric Constant 2.66
    @Frequency 2.00e+9 - 1.80e+10 Hz
    Dissipation Factor 0.0050
     
    Thermal PropertiesOriginal ValueComments
    Maximum Service Temperature, Air 350 °F
    Glass Transition Temp, Tg 166 °CResin, Wet, Cured at 450°F
     227 °CResin, Dry, Cured at 350°F

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Park Aerospace Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 7781 E-Glass Reinforced
    Saint-Gobain Quartzel® Fabric/Cyanate Ester Resin Composite
    Huntsman AroCy XU 71787.02 L Cyanate Ester
    Park Aerospace Nelco® N8000Q Cyanate Ester Epoxy Laminate and Prepreg
    Saint-Gobain Quartzel® Fiber/Cyanate Ester Resin Unidirectional Composite

    PRENEG03 / 138458

    Aluminum Castings

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.