MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Solvay IGEPAL® OD 410 Surfactant
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: Dispersant and emulsifier for cosmetic formulations

Identification: ETHYLENE GLYCOL PHENYL ETHER

C.T.F.A./INCI NAME: PHENOXYETHANOL

CAS: 122 – 99 – 6

Solubility: Insoluble in water, soluble in most polar and aromatic solvents.

Available in: Asia Pacific, Europe, Latin America and North America

Applications: Industrial formulations : Solvent for vinyl, phenolic, polyester, alkyd and cellulose acetate resins , ingredient of metal cleaners, paint strippers and cleaning compounds where solvents and solvent boosters are required , used as ink vehicle. Personal Care: Preservative. Polymer systems specialties: Intermediate for monomer synthesis.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.11 g/cc
 
Thermal PropertiesOriginal ValueComments
Melting Point 14.0 °CFreezing Point
Flash Point >= 100 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 24.0 Month
 
Component Elements PropertiesOriginal ValueComments
H2O, Water <= 0.50 %RPG16
 
Descriptive Properties
AppearanceLimpid liquidRPG31
Color<100 HUHazen, RPG23
CompositionActive1
 Phenol<0.2%, RPG42
 Phenol 1 E.O.>95%, RPG42
Ionic ChargeNonionic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay MACKAZOLINE® O-V Surfactant
Solvay MACKANATE® OPV Surfactant
Solvay MACKAM® 2CYSF Surfactant
Solvay MACKADET® EQ-178 Surfactant
Solvay JAGUAR® C 14 S Surfactant

WRHOD165 / 137396

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.