MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Hippe PC Polycarbonate  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: Hard, stiff, very good impact properties with a wide range of temperature (to -100°C). High stability of shape under heat. Clear with own slight yellowish color. Low water absorption, weather-resistant. Physiologically acceptable.

Information provided by Hippe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccDIN 53 479
Moisture Absorption at Equilibrium 0.15 %0.15 %Absorption of humidity in standard operating environment; DIN 53 715
Water Absorption at Saturation 0.35 %0.35 %DIN 53 495
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 100 MPa
@Time 30.0 sec
14500 psi
@Time 0.00833 hour
DIN 53 456
Tensile Strength 65.0 MPa9430 psiDIN 53 455
Elongation at Break 60 - 100 %60 - 100 %DIN 53 455
Tensile Modulus 2.20 GPa319 ksiDIN 53 457
Charpy Impact, Notched NBNBDIN 53 453
Coefficient of Friction, Dynamic 0.52 - 0.580.52 - 0.58Against steel, p=0.05 N/mm², v=0.6 m/s, hardened and ground
Abrasion 2222µm/km; Against steel, p=0.05 N/mm², v=0.6 m/s, hardened and ground
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+17 ohm-cm1.00e+17 ohm-cmDIN 53 482, VDE 0303, Part 3
Surface Resistance 1.00e+15 ohm1.00e+15 ohmDIN 53 482
Dielectric Constant 3.0
@Frequency 1e+6 Hz
3.0
@Frequency 1e+6 Hz
DIN 53 483, IEC-250
Dielectric Strength 27.0 kV/mm686 kV/inBreakdown; DIN 53 481, IEC-243, VDE 0303 Part 1
Dielectric Loss Index 0.0060
@Frequency 1e+6 Hz
0.0060
@Frequency 1e+6 Hz
DIN 53 483, IEC-250
 
Thermal PropertiesMetricEnglishComments
CTE, linear 60.0 - 70.0 µm/m-°C33.3 - 38.9 µin/in-°F
Specific Heat Capacity 1.20 J/g-°C0.287 BTU/lb-°F
Thermal Conductivity 0.190 W/m-K1.32 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 120 °C248 °FContinuous use
 140 °C284 °FShort Periods
Deflection Temperature at 0.46 MPa (66 psi) 140 °C284 °FISO-R 75 Method B
Deflection Temperature at 1.8 MPa (264 psi) 135 °C275 °FISO-R 75 Method A
Glass Transition Temp, Tg 145 °C293 °Fdynamic; DIN 53 736
Flammability, UL94 V-2V-2
 
Descriptive Properties
Colortransparent
Creep ResistanceGrade CTI 350DIN 53 480, IEC-112, VDE 0303 Part 1
Resistance to hot water, sudsnot resistant

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHIPPE980 / 121984

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.