MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex Sarlink® TPE ME-2240DB Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Sarlink ME-2200 series is a general purpose thermoplastic elastomer series, available in BLK, designed for exterior automotive molding applications. Sarlink ME-2240DB is a high hardness, low density, UV stabilized grade suitable for injection molding.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Chemical Resistant; Good Adhesion; Good Processability; Low Density; High Hardness; Low Specific Gravity; Light Stabilized; Low Flow; Lubricated; Sunlight Resistant; UV Resistant

Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Rubber Replacement

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding

Preliminary data. Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.928 g/ccISO 1183
Viscosity 203 cP
@Shear Rate 206 1/s,
Temperature 200 °C
ASTM D3835
Linear Mold Shrinkage 0.012 in/in48 hr, Injection Molded; ASTM D955
Linear Mold Shrinkage, Transverse 0.012 in/in48 hr, Injection Molded; ASTM D955
Melt Flow 12 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 38
@Time 15.0 sec
Injection Molded; ISO 868
 39
@Time 5.00 sec
Injection Molded; ISO 868
 44
@Time 1.00 sec
Injection Molded; ISO 868
 38.7
@Treatment Temp. 125 °C,
Time 15.0 sec
Change in Air, 168 hr; ISO 888
 39.3
@Treatment Temp. 125 °C,
Time 5.00 sec
Change in Air, 168 hr; ISO 888
 39.9
@Treatment Temp. 110 °C,
Time 15.0 sec
Change in Air, 1008 hr; ISO 888
 40
@Treatment Temp. 110 °C,
Time 5.00 sec
Change in Air, 1008 hr; ISO 888
 43.1
@Treatment Temp. 125 °C,
Time 1.00 sec
Change in Air, 168 hr; ISO 888
 45.7
@Treatment Temp. 110 °C,
Time 1.00 sec
Change in Air, 1008 hr; ISO 888
Tensile Strength at Break 1940 psiFlow, Type 1, 20 in/min; ISO 37
 2160 psiAcross Flow, Type 1, 20 in/min; ISO 37
 1770 psi
@Treatment Temp. 125 °C,
Time 605000 sec
Flow, Type 1, Change in Air; ISO 188
 1880 psi
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
Flow, Type 1, Change in Air; ISO 188
 2120 psi
@Treatment Temp. 125 °C,
Time 605000 sec
Across Flow, Type 1, Change in Air; ISO 188
 2130 psi
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
Across Flow, Type 1, Change in Air; ISO 188
Tensile Stress at Strain 889 psi
@Strain 100 %
Across Flow, Type 1, 20 in/min; ISO 37
 1060 psi
@Strain 100 %
Flow, Type 1, 20 in/min; ISO 37
Elongation at Break 630 %Flow, Type 1, 20 in/min; ISO 37
 720 %Across Flow, Type 1, 20 in/min; ISO 37
 64.8 %
@Treatment Temp. 125 °C,
Time 605000 sec
Across Flow, Type 1, Change in Air; ISO 188
 523 %
@Treatment Temp. 125 °C,
Time 605000 sec
Flow, Type 1, Change in Air; ISO 188
 567 %
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
Flow, Type 1, Change in Air; ISO 188
 694 %
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
Across Flow, Type 1, Change in Air; ISO 188
Tear Strength 340 pliFlow, Method Ba, Angle (Unnicked), 20 in/min; ISO 34-1
 380 pliAcross Flow, Method Ba, Angle (Unnicked), 20 in/min; ISO 34-1
Compression Set 37 %
@Temperature 22.8 °C,
Time 79200 sec
Type 1; ISO 815
 56 %
@Temperature 70.0 °C,
Time 79200 sec
Type 1; ISO 815
 68 %
@Temperature 90.0 °C,
Time 252000 sec
Type 1; ISO 815
 100 %
@Temperature 125 °C,
Time 252000 sec
Type 1; ISO 815
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 390 - 410 °F
Middle Barrel Temperature 400 - 420 °F
Front Barrel Temperature 410 - 430 °F
Nozzle Temperature 420 - 440 °F
Melt Temperature 420 - 440 °F
Mold Temperature 60.0 - 90.0 °F
Injection Pressure 200 - 800 psi
Back Pressure 25.0 - 125 psi
Cushion 0.150 - 1.00 in
Screw Speed 50 - 120 rpm
 
Descriptive Properties
AppearanceBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEKNQ1057 / 237548

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.