Mechanical Properties | Metric | English | Comments |
---|
Adhesive Bond Strength | 7.10 MPa @Temperature 150 °C | 1030 psi @Temperature 302 °F |
| 7.20 MPa @Temperature 150 °C | 1040 psi @Temperature 302 °F |
| 9.90 MPa @Temperature 180 °C | 1440 psi @Temperature 356 °F |
| 10.2 MPa @Temperature 180 °C | 1480 psi @Temperature 356 °F |
| 14.2 MPa @Temperature 120 °C | 2060 psi @Temperature 248 °F |
| 14.2 MPa @Temperature 80.0 °C | 2060 psi @Temperature 176 °F |
| 14.5 MPa @Temperature 120 °C | 2100 psi @Temperature 248 °F |
| 16.0 MPa @Temperature 150 °C | 2320 psi @Temperature 302 °F |
| 16.1 MPa @Temperature 150 °C | 2340 psi @Temperature 302 °F |
| 18.0 MPa @Temperature 22.8 °C | 2610 psi @Temperature 73.0 °F |
| 19.1 MPa @Temperature 80.0 °C | 2770 psi @Temperature 176 °F |
| 19.8 MPa @Temperature 120 °C | 2870 psi @Temperature 248 °F |
| 20.0 MPa @Temperature 120 °C | 2900 psi @Temperature 248 °F |
| 20.4 MPa @Temperature 22.8 °C | 2960 psi @Temperature 73.0 °F |
| 21.1 MPa @Temperature 135 °C | 3060 psi @Temperature 275 °F |
| 21.2 MPa @Temperature 22.8 °C | 3070 psi @Temperature 73.0 °F |
| 21.2 MPa @Temperature 22.8 °C | 3070 psi @Temperature 73.0 °F |
| 21.3 MPa @Temperature -8.89 °C | 3090 psi @Temperature 16.0 °F |
| 21.7 MPa @Temperature 80.0 °C | 3150 psi @Temperature 176 °F |
| 22.0 MPa @Temperature 22.8 °C | 3190 psi @Temperature 73.0 °F |
| 22.3 MPa @Temperature 22.8 °C | 3230 psi @Temperature 73.0 °F |
| 22.8 MPa @Temperature -8.89 °C | 3310 psi @Temperature 16.0 °F |
| 23.2 MPa @Temperature 22.8 °C | 3360 psi @Temperature 73.0 °F |
| 26.5 MPa @Temperature 80.0 °C | 3840 psi @Temperature 176 °F |
| 27.2 MPa @Temperature -55.0 °C | 3950 psi @Temperature -67.0 °F |
| 28.9 MPa @Temperature 22.8 °C | 4190 psi @Temperature 73.0 °F |
| 29.7 MPa @Temperature 80.0 °C | 4310 psi @Temperature 176 °F |
| 30.3 MPa @Temperature 22.8 °C | 4390 psi @Temperature 73.0 °F |
| 30.5 MPa @Temperature 22.8 °C | 4420 psi @Temperature 73.0 °F |
| 33.8 MPa @Temperature 22.8 °C | 4900 psi @Temperature 73.0 °F |
|
Thermal Properties | Metric | English | Comments |
---|
Glass Transition Temp, Tg | 111 °C | 232 °F |
| 119 °C | 246 °F |
| 180 °C | 356 °F |
| 193 °C | 379 °F |
|
Processing Properties | Metric | English | Comments |
---|
Cure Time | 90.0 min @Temperature 180 °C | 1.50 hour @Temperature 356 °F |
| 240 min @Temperature 150 °C | 4.00 hour @Temperature 302 °F |
|
Descriptive Properties |
---|
Climbing drum peel torque | 125 N/25mm |
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding
error. We also ask that you refer to MatWeb's
terms of use regarding this information.
Click here to view
all the property values for this datasheet as they were originally entered into MatWeb.