MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

American Black Gum (Black Tupelo) Wood
Categories: Wood and Natural Products; Wood; Hardwood

Material Notes: Diffuse-Porous Hardwood

Property values marked by an asterisk (*) have been taken from an unusually old reference source.

Key Words: Nyssa sylvatica; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.460 g/cc0.0166 lb/in³Oven Dry Weight/Unseasoned Volume
 0.721 g/cc0.0260 lb/in³Unseasoned*
 
Mechanical PropertiesMetricEnglishComments
Hardness, Wood Indentation 2800 N629 lb (f)Side. Force required to imbed a 0.444 inch steel ball to one-half its diameter
 3500 N787 lb (f)End. Force required to imbed a 0.444 inch steel ball to one-half its diameter
Tensile Strength, Ultimate 3.93 MPa570 psiPerpendicular to Grain*
Modulus of Rupture 0.0483 GPa7.00 ksiStatic Bending*
Flexural Yield Strength 27.6 MPa4000 psiFiber Stress at Elastic Limit; Static Bending*
Flexural Modulus 7.10 GPa1030 ksiStatic Bending*
Compressive Strength 4.14 MPa600 psiPerpendicular to Grain*
 16.8 MPa2440 psiParallel to Grain*
 21.0 MPa3040 psiMax Crushing Strength Parallel to Grain*
Shear Strength 7.58 MPa1100 psiParallel to Grain*
Impact 4.04.0in-lb/in³; Work to Elastic Limit; Unseasoned Sample; Impact Bending*
 98009800psi; Fiber Stress at Elastic Limit; Unseasoned Sample; Impact Bending*
Work to Elastic Limit 0.00627 J/cm³0.910 in-lb/in³Static Bending*
Work to Maximum Load 0.0552 J/cm³8.00 in-lb/in³Static Bending*
Cleavage 49.0 kN/m280 lb/inRadial surface of failure, Unseasoned*
 67.0 kN/m382 lb/inTangential surface of failure, Unseasoned*
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.124 W/m-K0.860 BTU-in/hr-ft²-°FOven Dry
 0.144 W/m-K1.00 BTU-in/hr-ft²-°F12% Moisture Content
Shrinkage 4.4 %4.4 %Radial; Unseasoned to Oven Dry*
 7.7 %7.7 %Tangential; Unseasoned to Oven Dry*
 13.3 %13.3 %Volumetric; Unseasoned to Oven Dry*

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
American Black Ash (Brown Ash) Wood
American Chestnut Wood
American Beech Wood
American Birch Wood
American Black Locust Wood

PTSA010 / 71239

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.