MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Covestro Bayhydrol® XP 2637 Polyurethane Coating
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings; Thermoset; Polyurethane, TS

Material Notes: Bayhydrol XP 2637 is a an ionic/non-ionic polycarbonate ester polyurethane dispersion. Bayhydrol XP 2637 is a solvent-free polyurethane dispersion which can be used to formulate coatings that harden at room temperature or baking coatings. It allows coating of a wide variety of substrates ranging from hard ones to flexible ones such as leather, textiles, plastics and metals. Coatings formulated with Bayhydrol XP 2637 exhibit high scratch resistance and lightfastness. Other benefits of Bayhydrol XP 2637 are good aging stability and very good hydrolysis resistance.

Properties / Applications: Bayhydrol XP 2637 is a solvent free polyurethane dispersion that can be used in the formulation of ambient-cure or bake coatings for a wide range of rigid and flexible substrates such as leather, vinyl- coated fabric, textiles, plastics and metals. Bayhydrol XP 2637 exhibits a combination of flexibility, good water and solvent resistance, outstanding hydrolytic stability and may be blended with other polyurethane dispersion to achieve intermediate properties. As with any product, use of Bayhydrol XP 2637 in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/cc
Volatiles 58 - 62 %1g/1h/125°C
pH 6.5 - 8.5
Viscosity <= 750 cPD= approx. 40 s-1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Samyang Trirex® 3025GN10 Polycarbonate, Reinforced Flame Retardancy
PTS Tristar® PC-20GF 20% Glass Reinforced Polycarbonate
PTS Tristar® PC-10GFR-(V) 10% Glass Reinforced UV Stabilized Polycarbonate With Release
Cadi C11000 ETP Standard Grade Copper

PCOVEST0188 / 201971

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.