MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Aperam Superimphy® 718 Bar-Corrosion application
Categories: Metal; Ferrous Metal

Material Notes: It is a precipitation-hardenable Ni-Cr alloy with a significant amount of Fe, Nb and Mo and containing lesser amounts of Al and Ti. This alloy combines excellent high strength up to 700°C with good corrosion resistance and excellent weldability. Exceptional creep-rupture strength at high temperature. It is a magnetic.

Applications:

  • Chemical industries
  • Safety parts
  • Power plant (gas turbine)
  • Oil and gas, petrochemistry
  • Aeronautic
Standards related to these applications: ASTM B637, NACE MR0175, AMS 5662

Information provided by Aperam

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Component Elements PropertiesOriginal ValueComments
Chromium, Cr 17 - 21 %
Iron, Fe 15.2 - 25.45 %
Molybdenum, Mo 2.8 - 3.3 %
Neodymium, Nd 4.75 - 5.5 %
Nickel, Ni 50 - 55 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Special Metals INCONEL® Alloy 718
MetalTek MTEK 718 Cast UNS N07718 Severe Corrosion and Heat Resistant Alloy
HP Alloys Alloy 718, 50% Cold Worked, Aged
HP Alloys Alloy 718, 50% Cold Worked
HP Alloys Alloy 718, 5% Cold Worked

NPERA023 / 194812

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.