MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Hyflon® AD 40H Perfluoropolymer
Categories: Polymer; Thermoplastic; Fluoropolymer

Material Notes: Hyflon® AD 40H is an amorphous perfluoro-polymer available in powder form.

Hyflon® AD polymers resemble semicrystalline perfluoropolymers in their performance properties as they exhibit high temperature stability, excellent hydrophobicity and chemical resistance as well as very low surface energy.

Key distinctive feature of Hyflon AD polymers is that they are soluble in selected solvents. In particular, their high solubility in perfluorinated solvents and their low solution viscosities make them suitable for solution process technologies.

Hyflon® AD can provide uniform and thin films or coatings (down to submicron thicknesses if required) by casting or coating techniques and thermal treatments, well below the typical baking temperatures of semicrystalline perfluoro-polymers.

Examples of typical applications include protective coatings, interlayer dielectric films and pellicles for electronics.

Main features of Hyflon® AD 40H include:
- Amorphous glassy polymer structure
- Solubility in perfluorinated solvent
- Low dielectric constant of 2.0 at 1 kHz
- Excellent optical properties
-- high UV transmittance
-- low refractive index

Applications: Coating Applications; Film

Features: Amorphous; Chemical Resistant; Good Thermal Stability

Safety and Toxicology
- Before using Hyflon fluoropolymer resins consult the product Material Safety Data Sheet and follow all label directions and handling precautions.
- As with all fluoropolymer materials, handling and processing should only be carried out in well ventilated areas. Vapor extractor units should be installed above processing equipment. Fumes must not be inhaled and eye and skin contact ought to be avoided. In case of skin contact, wash with soap and water. In case of eye contact flush with water immediately and seek medical help. Do not smoke in areas contaminated with powder, vapor or fumes. See Material Safety Data Sheet for detailed advice on waste disposal methods.

Storage and Handling
- Hyflon fluoropolymer resins can be stored without shelf life issues when kept in a clean and dry area at ambient temperatures. Opened containers should be tightly resealed to prevent dust contamination.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.98 g/ccASTM D792
Viscosity Test 1.3 dl/g
@Temperature 30.0 °C
Intrinsic Viscosity
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 90.0 °CASTM E1356
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.331ASTM D542
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
FormsPowder
ProcessingCoating; Solution Processing

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4242 / 280042

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.