MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Nouryon Perkadox 24L Polymer Dicetyl peroxydicarbonate
Categories: Other Engineering Material

Material Notes: Initiator for (co)polymerization of vinyl chloride, vinylidene chloride, acrylates and methacrylates. Used to increase melt strength of polypropylene to make high melt strength polypropylene (HMS-PP) by reactive extrusion process.

CAS number: 26322-14-5

EINECS/ELINCS No.: 247-611-0

Applications: Perkadox 24L is applied as an initiator for the suspension and mass polymerization of vinyl chloride in the temperature range between 45°C and 65°C. Perkadox 24L may be used in combination with other peroxides such as 1,1,3,3- Tetramethylbutyl peroxyneodecanoate (Trigonox 423), Cumyl peroxyneodecanoate (Trigonox 99) or Dilauroyl peroxide (Laurox) to increase reactor efficiency. Perkadox 24L has low water solubility, low vapor pressure and is quickly and evenly distributed into the monomer. There are important properties when a PVC resin of low fish-eye content and narrow particle size distribution is to be produced and autoclaves are to be kept free of crusts and scale.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.600 g/cc0.0217 lb/in³
Half-life  0.100
@Temperature 84.0 °C
0.100
@Temperature 183 °F
[hr]
 1.00
@Temperature 65.0 °C
1.00
@Temperature 149 °F
[hr]
 10.0
@Temperature 48.0 °C
10.0
@Temperature 118 °F
[hr]
Molecular Weight 570.9 g/mol570.9 g/mol
Storage Temperature <= 20.0 °C<= 68.0 °F
 
Thermal PropertiesMetricEnglishComments
Melting Point 52.0 °C126 °F
Decomposition Temperature 40.0 °C104 °FSelf-Accelerating Decomposition Temperature
 
Processing PropertiesMetricEnglishComments
Shelf Life 3.00 Month3.00 Month
 
Descriptive Properties
AppearanceWhite powder
Assay90.0-93.0 %
Content= 3000 mg/kgInorganic + organic hydrolysable chloride

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY767 / 286290

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.