MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Silon TABOREN PR 65 T 10S-089 Polypropylene, 10% Talc Reinforced
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 10% Talc Filler

Material Notes: TABOREN-PR 65 T 10S-089 is a compound based on mixture of polypropylene impact block copolymer and high density polyethylene, filled with 10% of talc and stabilized with a car interior UV/AOX additive package . It is scratch resistant and designed for injection molding of automotive interior applications with stress put on excellent processability and good surface performance.

Information provided by Silon US LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.980 g/cc0.0354 lb/in³ISO 1183-1
Melt Flow 13.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
13.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Storage Temperature <= 50.0 °C<= 122 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 17.0 MPa2470 psiISO 527
Elongation at Break 40.0 %40.0 %ISO 527
Flexural Modulus 1.30 GPa189 ksiISO 178
Charpy Impact Unnotched NBNBISO 179-1/1eU
Charpy Impact, Notched 2.00 J/cm²9.52 ft-lb/in²ISO 179-1/1eA
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 130 °C266 °Fmethod A50; ISO 306
 
Processing PropertiesMetricEnglishComments
Melt Temperature 200 - 250 °C392 - 482 °F
Mold Temperature 30.0 - 50.0 °C86.0 - 122 °F
Drying Temperature 80.0 °C
@Time 10800 sec
176 °F
@Time 3.00 hour
Injection Pressure 90.0 - 130 MPa13100 - 18900 psi
 
Descriptive Properties
AppearanceBlack
Processing Hold-on Pressure?40% of injection pressure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSILOM9863 / 325189

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.