MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

A. Schulman POLYBATCH™ AF-1085 Antifog Concentrate
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Description

POLYBATCH® AF-1085 is a 10% antifog concentrate based in LDPE. This concentrate is designed to provide excellent antifog performance in polyethylene film applications ranging from meat packaging to flowers and vegetables, which are stored in cold display cases. However, this product is not generally recommended for surface print applications. POLBATCH® AF-1085 is recommended for use at 6 to 10% addition levels depending upon customer specific requirements. Higher usage levels may be required depending upon film thickness or multilayer package design

Information provided by A. Schulman.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.940 g/cc0.940 g/ccASTM D792
Moisture Absorption <= 0.200 %<= 0.200 %190°C; ASTM D789
Additive Loading 10 %10 %
Melt Flow 15 g/10 min
@Load 2.16 kg,
Temperature 190 °C
15 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Descriptive Properties
Pellet Count 70pellets/gram

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman POLYBATCH™ ASP-2000 Permanent Antistatic Product
A. Schulman POLYBATCH™ ASC-331 Inorganic Antislip Masterbatch Based in Polyethylene
A. Schulman POLYBLAK™ 4651SF Universal Black Color Concentrate, 50% Carbon Black in EVA
A. Schulman POLYBATCH™ White 8750 Concentrate Based In HDPE
Chevron Phillips Marlex® HHM TR-305 Medium density hexene copolymer

PASHU363 / 25327

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.