MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
TIMCAL TIMREX® KS150 Primary Synthetic Graphite
Categories: Carbon; Graphite; Other Engineering Material; Additive/Filler for Polymer

Material Notes: TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all production and processing stages, strict final inspection, and clearly defined development processes.

TIMREX Primary Synthetic Graphite shows unique properties thanks to the combination of a consistent purity, perfect crystalline structure and well defined texture.

Tribological and mechanical properties:

  • Medium toughness
  • Good lubrication properties
Advantages and applications:
  • Low friction coefficient
  • Low wear of the counterpart
  • Good transfer-film formation
  • High electrical conductivity
  • Suitable for pitch-bonded and resin-bonded brushes
  • Copper/bronze bearings
  • Copper friction parts copper clutch facings
Information provided by TIMCAL

Key Words: CAS Number 7782-42-5
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.420 g/ccScott
 0.510 g/ccTap
Particle Size 5.0 µmSpringback 11.5%, pressure 0.477 t/cc
 20 µmSpringback 13%, pressure 0.477 t/cc
 >= 63 µmd50, 40%, Vibrated sieving
 75 µmSpringback 17%, pressure 0.477 t/cc
 >= 100 µmd90, 20%, Vibrated sieving
 <= 180 µm>95%, Guaranteed
 >= 180 µm0.2%
 550 µmat a density of 2.16 g/cc
 1000 µmat a density of 2.12 g/cc
Specific Surface Area 3.0 m²/gBET
Deformation 1.4 %plastic
 1.4 %elastic
 2.8 %plastic + elastic
Ash 0.060 %Typical
 <= 0.10 %Guaranteed
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.55 ohm-cmparticle size 80 um, pressure 2.5 t/cc
 1.60 ohm-cmparticle size 42 um, pressure 2.5 t/cc
 1.80 ohm-cmparticle size 15 um, pressure 2.5 t/cc
 2.25 ohm-cmparticle size 10 um, pressure 2.5 t/cc
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 140 W/m-K
 
Component Elements PropertiesOriginal ValueComments
H2O, Water 0.050 %Typical
 <= 0.50 %Guaranteed
 
Descriptive Properties
Crystallite height Lc>100 nm
DBP absorption52 g/100g(Dibutylphthalate)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
TIMCAL TIMREX® KS44 Primary Synthetic Graphite
TIMCAL TIMREX® KS15 Primary Synthetic Graphite
TIMCAL TIMREX® KS75 Primary Synthetic Graphite
TIMCAL TIMREX® T75 Primary Synthetic Graphite
TIMCAL TIMREX® KS500 Primary Synthetic Graphite

CTIMCAL16 / 2658

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.